The YES EcoClean system is an ICP downstream asher used for the removal of resist and other organic. 4" wafers are cassette loaded or smaller samples are loaded onto 4" carriers into the system. Samples can be heated from ~120C to 200C by controlling the sample height via the lift pins during process, while being exposed to ICP-cracked oxygen to remove organic materials. The excitation of the oxygen is done remotely and a baffle keeps ions from reaching the surface. Radicals diffuse and are scattered across the wafer surface for efficient cleaning and PR removal without any ion damage. Resist etch rates of multiple microns per minute can be achieved. See the process pages below for etch recipes for various resist removal recipes. |
The YES EcoClean system is an ICP downstream asher used for the removal of resist and other organic. 4" wafers are cassette loaded or smaller samples are loaded onto 4" carriers into the system. Samples can be heated from ~120C to 200C by controlling the sample height via the lift pins during process, while being exposed to ICP-cracked oxygen to remove organic materials. The excitation of the oxygen is done remotely and a baffle keeps ions from reaching the surface. Radicals diffuse and are scattered across the wafer surface for efficient cleaning and PR removal without any ion damage. Resist etch rates of multiple microns per minute can be achieved. See the process pages below for etch recipes for various resist removal recipes. |
||
| Line 18: | Line 18: | ||
[https://www.yieldengineering.com/Products/Plasma-Strip-Descum-Systems/YES-%C3%89coClean YES EcoClean Manufacturer Page] |
[https://www.yieldengineering.com/Products/Plasma-Strip-Descum-Systems/YES-%C3%89coClean YES EcoClean Manufacturer Page] |
||
== Documentation == |
|||
* YES Plasma Strip System Standard Operating Procedure |
|||
Revision as of 14:57, 25 September 2019
| ||||||||||||||||||||
About
The YES EcoClean system is an ICP downstream asher used for the removal of resist and other organic. 4" wafers are cassette loaded or smaller samples are loaded onto 4" carriers into the system. Samples can be heated from ~120C to 200C by controlling the sample height via the lift pins during process, while being exposed to ICP-cracked oxygen to remove organic materials. The excitation of the oxygen is done remotely and a baffle keeps ions from reaching the surface. Radicals diffuse and are scattered across the wafer surface for efficient cleaning and PR removal without any ion damage. Resist etch rates of multiple microns per minute can be achieved. See the process pages below for etch recipes for various resist removal recipes.
YES EcoClean Manufacturer Page
Documentation
- YES Plasma Strip System Standard Operating Procedure