Automated Coat/Develop System (S-Cubed Flexi): Difference between revisions

From UCSB Nanofab Wiki
Jump to navigation Jump to search
Content deleted Content added
m fixed ToolTemplate 'type' arg
added ToolID (link to SUM)
Line 8: Line 8:
|type = Wet Processing
|type = Wet Processing
|recipe = Lithography
|recipe = Lithography
|materials =
|materials =
|toolid=
|toolid=67
}}
}}
'''THIS TOOL IS ONLY FOR STAFF USE AT THIS TIME.'''
'''THIS TOOL IS ONLY FOR STAFF USE AT THIS TIME.'''

Revision as of 20:29, 13 November 2019

Automated Coat/Develop System (S-Cubed Flexi)
Tool Type Wet Processing
Location Bay 7
Supervisor Tony Bosch
Supervisor Phone (805) 893-3486
Supervisor E-Mail bosch@ece.ucsb.edu
Description Automatic Coat/Bake/Develop
Manufacturer S-Cubed
Model Flexi (Custom)
Wet Processing Recipes
Sign up for this tool


THIS TOOL IS ONLY FOR STAFF USE AT THIS TIME.

About

To Be Added

Detailed Specifications

  • Wafer Size: 100mm (150mm possible but not set up)
  • PR Coating Properties:
    • Uniformity < 1.0%
    • < 100 particles on 100mm wafer
  • Photoresists/Underlayers Available:
    • UV6-0.8
    • DS-K101-304
    • PMMA
    • PMGI SF11
    • PMGI SF5
  • Solvents Available:
    • EBR100
  • Developers Available:
    • AZ 300 MiF

Process Information

Operating Procedures

  • To Be Added