Automated Coat/Develop System (S-Cubed Flexi): Difference between revisions

From UCSB Nanofab Wiki
Jump to navigation Jump to search
Content deleted Content added
Text replacement - "www.nanotech.ucsb.edu/wiki/" to "wiki.nanotech.ucsb.edu/wiki/"
added link to SOP
Line 15: Line 15:
=About=
=About=


The S3 is a Coater/Developer system that has 4 hotplates each with independent temperature control and a chill plate. A central robot picks your wafer/s from a cassette, processes them and returns them to the cassette. The system is recipe driven with a high degree of process control and minimal backside contamination. At this time only full size substrates are allowed on this system. The S3 Coater is still in process development and not open for general use.
The S3-Coater is a Coater/Developer system that has one photoresist spinner, one developer spinner and 4 hotplates each with independent temperature control and a chill plate. A central robot picks your wafer/s from one of 2 cassettes, processes them and returns them to the cassette. The system is recipe driven with a high degree of process control and minimal backside contamination, and coats photoresists with low particle counts/streaks and high uniformity.

At this time only full size substrates are allowed on this system. The S3 Coater is still in process development and not open for general use.


=Detailed Specifications=
=Detailed Specifications=
Line 41: Line 43:
=Operating Procedures=
=Operating Procedures=


*[[S-Cubed Flexi - Operating Procedure|Standard Operating Procedure]] - For running pre-written recipes only.
*''To Be Added''

Revision as of 18:42, 26 August 2020

Automated Coat/Develop System (S-Cubed Flexi)
Tool Type Wet Processing
Location Bay 7
Supervisor Tony Bosch
Supervisor Phone (805) 893-3486
Supervisor E-Mail bosch@ece.ucsb.edu
Description Automatic Coat/Bake/Develop
Manufacturer S-Cubed
Model Flexi (Custom)
Wet Processing Recipes
Sign up for this tool


THIS TOOL IS ONLY FOR STAFF USE AT THIS TIME.

About

The S3-Coater is a Coater/Developer system that has one photoresist spinner, one developer spinner and 4 hotplates each with independent temperature control and a chill plate. A central robot picks your wafer/s from one of 2 cassettes, processes them and returns them to the cassette. The system is recipe driven with a high degree of process control and minimal backside contamination, and coats photoresists with low particle counts/streaks and high uniformity.

At this time only full size substrates are allowed on this system. The S3 Coater is still in process development and not open for general use.

Detailed Specifications

  • Wafer Size: 100mm (150mm possible but not set up)
  • PR Coating Properties:
    • Uniformity < 1.0%
    • < 100 particles on 100mm wafer
  • Photoresists/Underlayers Available:
    • UV6-0.8
    • DS-K101-304
    • PMMA
    • PMGI SF11
    • PMGI SF5
  • Solvents Available:
    • EBR100
  • Developers Available:
    • AZ 300 MiF

Process Information

Operating Procedures