Thermal evaporator #2 is the designated "Solder" evaporator. The tool is used primarily for solder materials including Gold, Indium and Tin. |
Thermal evaporator #2 is the designated "Solder" evaporator. The tool is used primarily for solder materials including Gold, Indium and Tin. See the Recipes section below for other materials used. |
||
Use this tool for materials with low melting temperatures, or for materials that have a high risk of contamination in the e-beam evaporators. |
Use this tool for materials with low melting temperatures, or for materials that have a high risk of contamination in the e-beam evaporators. |
||
| Line 24: | Line 24: | ||
== Recipes == |
== Recipes == |
||
* [[Thermal Evaporation Recipes#Thermal Evaporator 2|Recipes > Thermal Evaporation Recipes > Thermal Evaporator 2]] |
* [[Thermal Evaporation Recipes#Thermal Evaporator 2|Recipes > Thermal Evaporation Recipes > Thermal Evaporator 2]] |
||
** ''Visit this page for the materials |
** ''Visit this page for the materials table and evaporation parameters for all materials available.'' |
||
Revision as of 16:27, 19 May 2020
| |||||||||||||||||||||
About
Thermal evaporator #2 is the designated "Solder" evaporator. The tool is used primarily for solder materials including Gold, Indium and Tin. See the Recipes section below for other materials used.
Use this tool for materials with low melting temperatures, or for materials that have a high risk of contamination in the e-beam evaporators.
Detailed Specifications
Wafers up to 12" can be mounted.