Dicing Saw (ADT): Difference between revisions
Jump to navigation
Jump to search
Content deleted Content added
Text replacement - "/wiki/index.php" to "/w/index.php" |
Updated SOP Rev |
||
| Line 10: | Line 10: | ||
|toolid=49 |
|toolid=49 |
||
}} |
}} |
||
== |
==About== |
||
The ADT 7100 Dicing Saw is optimized for multi-angle dicing of thin, tight tolerance products up to 200 mm x 200 mm. It is currently setup for dicing up to 8” diameter wafers. Check the [https://wiki.nanotech.ucsb.edu/w/index.php?title=Packaging_Recipes#Dicing_Saw_Recipes_.28ADT_7100.29 Dicing Saw Recipes page] for the blades we currently stock. |
The ADT 7100 Dicing Saw is optimized for multi-angle dicing of thin, tight tolerance products up to 200 mm x 200 mm. It is currently setup for dicing up to 8” diameter wafers. Check the [https://wiki.nanotech.ucsb.edu/w/index.php?title=Packaging_Recipes#Dicing_Saw_Recipes_.28ADT_7100.29 Dicing Saw Recipes page] for the blades we currently stock. |
||
| Line 17: | Line 17: | ||
Contact the tool supervisor for blades and dicing frames for your group. |
Contact the tool supervisor for blades and dicing frames for your group. |
||
== |
==Detailed Specifications== |
||
== |
==Operating Procedures== |
||
| ⚫ | |||
| ⚫ | |||
| ⚫ | |||
| ⚫ | |||
| ⚫ | |||
| ⚫ | |||
| ⚫ | |||
| ⚫ | |||
| ⚫ | |||
| ⚫ | |||
| ⚫ | |||
| ⚫ | |||
| ⚫ | |||
| ⚫ | |||
Be sure to also see the recipes for protecting your sample from dicing dust, and mounting/unmounting. |
Be sure to also see the recipes for protecting your sample from dicing dust, and mounting/unmounting. |
||
Revision as of 19:40, 9 September 2021
|
About
The ADT 7100 Dicing Saw is optimized for multi-angle dicing of thin, tight tolerance products up to 200 mm x 200 mm. It is currently setup for dicing up to 8” diameter wafers. Check the Dicing Saw Recipes page for the blades we currently stock.
An ADT WM-966 tape applicator & Ultron Systems UH104-8 UV lamp system is used to apply UV-release tape for securing die during dicing.
Contact the tool supervisor for blades and dicing frames for your group.
Detailed Specifications
Operating Procedures
- ADT Dicing Saw Standard Operating Procedure
- Setting up the Saw before Cutting - Disregard and refer to SOP above
- Standard Dicing Procedure - Programmed Cut Map
- Standard Dicing Procedure - Single Cuts
- Recovering an Old Recipe
Recipes
- Recipes > Packaging > Dicing Saw Recipes (ADT 7100)
Be sure to also see the recipes for protecting your sample from dicing dust, and mounting/unmounting.