ICP Etch 2 (Panasonic E626I): Difference between revisions

From UCSB Nanofab Wiki
Jump to navigation Jump to search
Content deleted Content added
→Recipes: separate Process Control section/link
Line 42: Line 42:
=Recipes=
=Recipes=


*[https://wiki.nanotech.ucsb.edu/w/index.php?title=ICP_Etching_Recipes#ICP_Etch_2_.28Panasonic_E640.29 '''ICP2 Etching Recipes''']
*'''Recipes > Dry Etch >''' [https://wiki.nanotech.ucsb.edu/w/index.php?title=ICP_Etching_Recipes#ICP_Etch_2_.28Panasonic_E640.29 '''<u>ICP2 Etching Recipes</u>''']
**Starting point recipes for ICP2 specifically.
**Starting point recipes for ICP2 specifically.
*[[ICP Etching Recipes#Process Control Data .28Panasonic 2.29|Process Control Data]]
*[[ICP Etching Recipes#Process Control Data .28Panasonic 2.29|Process Control Data]]
**''Historical Data'' records "calibration" etches to test tool performance.
**Historical Data records "calibration" etches to test tool performance.


*[https://wiki.nanotech.ucsb.edu/w/index.php?title=Dry_Etching_Recipes Dry Etching Recipes]
*'''Recipes > [https://wiki.nanotech.ucsb.edu/w/index.php?title=Dry_Etching_Recipes <u>Dry Etching Recipes</u>]'''
**Table of all dry etching recipes, showing '''etched materials vs. tool''' etc.
**Table of all dry etching recipes, showing '''etched materials vs. tool''' etc.

Revision as of 20:49, 11 February 2022

ICP Etch 2 (Panasonic E626I)
Tool Type Dry Etch
Location Bay 2
Supervisor Tony Bosch
Supervisor Phone (805) 893-3486
Supervisor E-Mail bosch@ece.ucsb.edu
Description ICP Etch
Manufacturer Panasonic Factory Solutions
Dry Etch Recipes
Sign up for this tool


About

This is a single-chamber tool for etching of a variety of materials. The chamber is configured as an ICP etching tool with 1000 W ICP power, 500 W RF substrate power, and RT - 80°C operation with back-side He cooling and an electrostatic chuck to maintain controlled surface temperatures during etching. This chamber has Cl2, BCl3, CF4, CHF3, SF6, Ar, N2, and O2 for gas sources and can be used to etch a variety of materials from SiO2 to metals to compound semiconductors. The chamber is evacuated with a 2000 lpm Osaka Vacuum magnetically levitated turbo pump, allowing for fast pump down.

The system is also equipped with a red laser monitoring system from Intellemetrics for more precise etch stop control.

Detailed Specifications

  • 1000 W ICP source, 500 W RF Sample Bias Source in etching chamber
  • Room Temp. – 80°C sample temperature for etching. Default 15°C Chuck temperature.
  • Optimal Emission Monitoring
  • Etch pressure from 0.1 Pa to 5 Pa (0.75 mT - 37.5 mT)
  • Cl2, BCl3, (Ar or CHF3), (CF4 or SF6), N2, and O2 in etch chamber
  • O2, N2, CF4, H2O Vapor for ashing chamber
  • Single 6” diameter wafer capable system
  • Pieces possible by mounting to 6” wafer
  • 670nm laser endpoint detector with camera and simulation software: Intellemetrics LEP 500

Documentation

Recipes

  • Recipes > Dry Etching Recipes
    • Table of all dry etching recipes, showing etched materials vs. tool etc.