''This Tool is now available for training - please contact the supervisor. 2022-11-01''
''This Tool is now available for training - please contact the supervisor. 2022-11-01''


=About=
==About==


The S3-Coater is a Coater/Developer system that has one photoresist spinner, one developer spinner and 4 hotplates each with independent temperature control and a chill plate. A central robot picks your wafer/s from one of 2 cassettes, processes them and returns them to the cassette. The system is recipe driven with a high degree of process control and minimal backside contamination, and coats photoresists with low particle counts/streaks and high uniformity.
The S3-Coater is a Coater/Developer system that has one photoresist spinner, one developer spinner and 4 hotplates each with independent temperature control and a chill plate. A central robot picks your wafer/s from one of 2 cassettes, processes them and returns them to the cassette. The system is recipe driven with a high degree of process control and minimal backside contamination, and coats photoresists with low particle counts/streaks and high uniformity.
Line 20: Line 20:
At this time only full size substrates are allowed on this system. The S3 Coater is still in process development and not open for general use.
At this time only full size substrates are allowed on this system. The S3 Coater is still in process development and not open for general use.


=Detailed Specifications=
==Detailed Specifications==


*Wafer Size: 100mm (150mm possible but not set up)
*Wafer Size: 100mm (150mm possible but not set up)
Line 27: Line 27:
**< 100 particles on 100mm wafer
**< 100 particles on 100mm wafer
*Photoresists/Underlayers Available:
*Photoresists/Underlayers Available:
**UV6-0.8
**UV6-0.8
**DS-K101-304
**DS-K101-304
**PMMA - '''<u>NOT FOR PUBLIC USE AT THIS TIME</u>'''
**PMMA - '''<u>NOT FOR PUBLIC USE AT THIS TIME</u>'''
Line 37: Line 37:
**AZ 300 MiF - '''<u>NOT FOR GENERAL USE AT THIS TIME</u>'''
**AZ 300 MiF - '''<u>NOT FOR GENERAL USE AT THIS TIME</u>'''


=Process Information=
==Process Information==


*Recipe Page for S-Cubed Coater: [[Lithography Recipes#Automated%20Coat.2FDevelop%20System%20Recipes%20.28S-Cubed%20Flexi.29|Lithography Recipes > Automated Coat/Develop System Recipes (S-Cubed Flexi]])
*Recipe Page for S-Cubed Coater: [[Lithography Recipes#Automated%20Coat.2FDevelop%20System%20Recipes%20.28S-Cubed%20Flexi.29|Lithography Recipes > Automated Coat/Develop System Recipes (S-Cubed Flexi]])
*See the [https://wiki.nanotech.ucsb.edu/w/index.php?title=Lithography_Recipes#Chemicals_Stocked_.2B_Datasheets Photolith. Chemicals page] for info on the installed resists.
*See the [https://wiki.nanotech.ucsb.edu/w/index.php?title=Lithography_Recipes#Chemicals_Stocked_.2B_Datasheets Photolith. Chemicals page] for info on the installed resists.


=Operating Procedures=
==Operating Procedures==


**[[S-Cubed Flexi - Operating Procedure|Standard Operating Procedure]] - For running pre-written recipes only.
**[[S-Cubed Flexi - Operating Procedure|Standard Operating Procedure]] - For running pre-written recipes only.

== Recipes ==
'''Recipes > Lithography >''' [[Lithography Recipes#Automated Coat.2FDevelop System Recipes .28S-Cubed Flexi.29|'''<u>Automated Coater Recipes</u>''']] - See all available spin-coat recipes for this machine. Only Staff may edit/create recipes.

Revision as of 21:41, 8 November 2022

Automated Coat/Develop System (S-Cubed Flexi)
Location Bay 7
Tool Type Wet Processing
Manufacturer S-Cubed
Model Flexi (Custom)
Description Automatic Coat/Bake/Develop

Primary Supervisor Tony Bosch
(805) 893-3486
bosch@ece.ucsb.edu

Secondary Supervisor

Lee Sawyer


Recipes Wet Processing Recipes

SignupMonkey: Sign up for this tool


This Tool is now available for training - please contact the supervisor. 2022-11-01

About

The S3-Coater is a Coater/Developer system that has one photoresist spinner, one developer spinner and 4 hotplates each with independent temperature control and a chill plate. A central robot picks your wafer/s from one of 2 cassettes, processes them and returns them to the cassette. The system is recipe driven with a high degree of process control and minimal backside contamination, and coats photoresists with low particle counts/streaks and high uniformity.

At this time only full size substrates are allowed on this system. The S3 Coater is still in process development and not open for general use.

Detailed Specifications

  • Wafer Size: 100mm (150mm possible but not set up)
  • PR Coating Properties:
    • Uniformity < 1.0%
    • < 100 particles on 100mm wafer
  • Photoresists/Underlayers Available:
    • UV6-0.8
    • DS-K101-304
    • PMMA - NOT FOR PUBLIC USE AT THIS TIME
    • PMGI SF11 - NOT FOR GENERAL USE AT THIS TIME
    • PMGI SF5 - NOT FOR GENERAL USE AT THIS TIME
  • Solvents Available:
    • EBR100 (wafer backside cleaning)
  • Developers Available:
    • AZ 300 MiF - NOT FOR GENERAL USE AT THIS TIME

Process Information

Operating Procedures

Recipes

Recipes > Lithography > Automated Coater Recipes - See all available spin-coat recipes for this machine. Only Staff may edit/create recipes.