Template:Announcements: Difference between revisions
Jump to navigation
Jump to search
Content deleted Content added
mNo edit summary |
ASML Down: laser fail |
||
| Line 14: | Line 14: | ||
<!------------- Equipment Status ----------------> |
<!------------- Equipment Status ----------------> |
||
===== ASML: Down |
===== ASML: Down for Laser Hardware Failure ===== |
||
The DUV Laser has a failed component, we are awaiting parts for repair. |
|||
On Dec 12th the system will be down for half a day starting at ~12n, so we can perform periodic maintenance (PM) on the DUV Laser. |
|||
// [[User:John d|John d]] |
// [[User:John d|John d]] 06:53, 13 December 2022 (PST) |
||
===== Au Plating: DOWN ===== |
===== Au Plating: DOWN ===== |
||
Revision as of 14:53, 13 December 2022
Important Announcements
ASML: Down for Laser Hardware Failure
The DUV Laser has a failed component, we are awaiting parts for repair. // John d 06:53, 13 December 2022 (PST)
Au Plating: DOWN
Bath damaged, system is down for repair. // John d 08:48, 27 October 2022 (PDT)
E-Beam#2: Heater UP
We tested the heater to 680°C three times without any issues. There is still the issue with the temp controller not communicating with the software which will get sorted out eventually. In the meantime you will just change the temp using the controller, directions are posted at the tool. // John d 15:55, 6 December 2022 (PST)
NanoFab Job Openings
The NanoFab has current job openings, apply at: NanoFab Job Postings
// John d 23:55, 4 October 2022 (PDT)