Process Group - Process Control Data: Difference between revisions

From UCSB Nanofab Wiki
Jump to navigation Jump to search
Content deleted Content added
→Etching (Process Control Data): FL-ICP example chart with link to live charts
Line 44: Line 44:


*[https://docs.google.com/spreadsheets/d/15hYkCqL3UNNayt4sXrvVi4mBj-OSdnF7PE29mQW9AEY/edit?usp=sharing SiO<sub>2</sub> Etching with CHF3/CF4 - '''Etch Data''']
*[https://docs.google.com/spreadsheets/d/15hYkCqL3UNNayt4sXrvVi4mBj-OSdnF7PE29mQW9AEY/edit?usp=sharing SiO<sub>2</sub> Etching with CHF3/CF4 - '''Etch Data''']
*[https://docs.google.com/spreadsheets/d/15hYkCqL3UNNayt4sXrvVi4mBj-OSdnF7PE29mQW9AEY/edit#gid=1804752281 SiO<sub>2</sub> Etching with CHF3/CF4 - '''Plots''']
*[https://docs.google.com/spreadsheets/d/15hYkCqL3UNNayt4sXrvVi4mBj-OSdnF7PE29mQW9AEY/edit#gid=1804752281 SiO<sub>2</sub> Etching with CHF3/CF4 - '''Plots'''][[File:FL-ICP Process Control Data Example.jpg|alt=example of Process Control Charts|none|thumb|242x242px|[https://docs.google.com/spreadsheets/d/15hYkCqL3UNNayt4sXrvVi4mBj-OSdnF7PE29mQW9AEY/edit#gid=1804752281 Click for Process Control Charts]|link=https://docs.google.com/spreadsheets/d/15hYkCqL3UNNayt4sXrvVi4mBj-OSdnF7PE29mQW9AEY/edit#gid=1804752281]]


==== OLD Process Control Data ====
====OLD Process Control Data====


*[[Test Data of Etching SiO2 with CHF3/CF4-Fluorine ICP Etcher|SiO<sub>2</sub> Etching with CHF3/CF4 (FL-ICP]]) - ''No data prior to 2023-01-20''
*[[Test Data of Etching SiO2 with CHF3/CF4-Fluorine ICP Etcher|SiO<sub>2</sub> Etching with CHF3/CF4 (FL-ICP]]) - ''No data prior to 2023-01-20''
Line 52: Line 52:
===[[ICP Etching Recipes#Process Control Data .28Panasonic 1.29|Panasonic ICP #1]]===
===[[ICP Etching Recipes#Process Control Data .28Panasonic 1.29|Panasonic ICP #1]]===


*[https://docs.google.com/spreadsheets/d/1gBqCYXSl7IqpNL-yI11cuURlfZpTWwXUVM9hY_gGpT8/edit?usp=sharing SiO<sub>2</sub> Etch with CHF<sub>3</sub>/CF<sub>4</sub> - '''Etch Data''']
*[[Test Data of etching SiO2 with CHF3/CF4-ICP1|SiO2 Etching with CHF3/CF4 - ICP1]]
*[https://docs.google.com/spreadsheets/d/1gBqCYXSl7IqpNL-yI11cuURlfZpTWwXUVM9hY_gGpT8/edit#gid=1804752281 SiO<sub>2</sub> Etch with CHF<sub>3</sub>/CF<sub>4</sub> - '''Plots''']

[[File:ICP1 Process Control Data Example.jpg|alt=example chart of ICP1 SiO2 Process Control Chart|none|thumb|250x250px|[https://docs.google.com/spreadsheets/d/1gBqCYXSl7IqpNL-yI11cuURlfZpTWwXUVM9hY_gGpT8/edit#gid=1804752281 Click for Process Control Charts]|link=https://docs.google.com/spreadsheets/d/1gBqCYXSl7IqpNL-yI11cuURlfZpTWwXUVM9hY_gGpT8/edit#gid=1804752281]]

==== Old Process Control Data ====

* [[Test Data of etching SiO2 with CHF3/CF4-ICP1|SiO<sub>2</sub> Etch with CHF<sub>3</sub>/CF<sub>4</sub> (Panasonic 1)]] - ''No data prior to 2023-01-20''


===[[ICP Etching Recipes#Process Control Data .28Panasonic 2.29|Panasonic ICP#2]]===
===[[ICP Etching Recipes#Process Control Data .28Panasonic 2.29|Panasonic ICP#2]]===

Revision as of 19:28, 20 January 2023

These are the same links found on individual tool pages, in the Recipes > <<tool page>> > Process Control section.

Deposition (Process Control Data)

PECVD #1 (PlasmaTherm 790)

PECVD #2 (Advanced Vacuum)

ICP-PECVD (Unaxis VLR Dep)

Ion Beam Sputter Deposition (Veeco Nexus)

Old Data (Pre 2022)

Old data in a different format can be found below:

Etching (Process Control Data)

PlasmaTherm SLR Fluorine Etcher

OLD Process Control Data

Panasonic ICP #1

example chart of ICP1 SiO2 Process Control Chart
Click for Process Control Charts

Old Process Control Data

Panasonic ICP#2

Unaxis VLR Etch

Oxford PlasmaPro Cobra Etcher