Process Group - Process Control Data: Difference between revisions

From UCSB Nanofab Wiki
Jump to navigation Jump to search
Content deleted Content added
m Litho to Top of page, link to ASML recipes page
→Stepper #3 (ASML DUV): included example images
Line 10: Line 10:
*[https://docs.google.com/spreadsheets/d/1xW1TFH_QjPMWl9T1jiKzwmYe4B2wg7KY-nqOKUoXttI/edit#gid=0 '''Data for CD Uniformity and Particulate Contamination''']
*[https://docs.google.com/spreadsheets/d/1xW1TFH_QjPMWl9T1jiKzwmYe4B2wg7KY-nqOKUoXttI/edit#gid=0 '''Data for CD Uniformity and Particulate Contamination''']


:{|
|[[File:ASML CD Cals - Example Table.jpg|alt=ASML CD Calibration data - Screenshot of Table|none|thumb|300x300px|''Example of Data Table with SEM's of 320nm features. [https://docs.google.com/spreadsheets/d/1xW1TFH_QjPMWl9T1jiKzwmYe4B2wg7KY-nqOKUoXttI/edit#gid=0 Click for full data table.]''|link=https://docs.google.com/spreadsheets/d/1xW1TFH_QjPMWl9T1jiKzwmYe4B2wg7KY-nqOKUoXttI/edit#gid=0]]
|[[File:ASML CD Cals - Example Plot.jpg|alt=ASML CD Calibration Data - Screenshot of SPC Plot|none|thumb|''Example SPC Chart - Measured Critical Dimension "CD" versus Date. [https://docs.google.com/spreadsheets/d/1xW1TFH_QjPMWl9T1jiKzwmYe4B2wg7KY-nqOKUoXttI/edit#gid=1804752281 Click for charts.]''|link=https://docs.google.com/spreadsheets/d/1xW1TFH_QjPMWl9T1jiKzwmYe4B2wg7KY-nqOKUoXttI/edit#gid=1804752281]]
|}


<hr style="height:5px">
<hr style="height:5px">
<hr style="height:5px">
<hr style="height:5px">

=Deposition (Process Control Data)=
=Deposition (Process Control Data)=
''Process Control data for various deposition tools in the lab.''
''Process Control data for various deposition tools in the lab.''

Revision as of 23:41, 18 May 2023

These are the same links found on individual tool pages, in the Recipes > <<tool page>> > Process Control section.

Lithography (Process Control Data)

Process Control Data for Nanofab Lithography/patterning tools.

Stepper #3 (ASML DUV)

ASML CD Calibration data - Screenshot of Table
Example of Data Table with SEM's of 320nm features. Click for full data table.
ASML CD Calibration Data - Screenshot of SPC Plot
Example SPC Chart - Measured Critical Dimension "CD" versus Date. Click for charts.


Deposition (Process Control Data)

Process Control data for various deposition tools in the lab.

PECVD #1 (PlasmaTherm 790)

PECVD #2 (Advanced Vacuum)

ICP-PECVD (Unaxis VLR Dep)

Ion Beam Sputter Deposition (Veeco Nexus)

Old Data (Pre 2022)

Old data in a different format can be found below:




Etching (Process Control Data)

Process Control data for various dry etching tools in the lab.

PlasmaTherm SLR Fluorine Etcher

OLD Process Control Data

Panasonic ICP #1

Old Process Control Data

Panasonic ICP#2

Old Process Control Data

Unaxis VLR Etch

Oxford PlasmaPro Cobra Etcher

Calibration / Process testing data taken using the "InP Ridge Etch" process: Cl2/CH4/H2 @ 60°C, 1cm piece with ~50% SiO2 hardmask.

Old Process Control Data