ICP Etching Recipes: Difference between revisions
Jump to navigation
Jump to search
Content deleted Content added
No edit summary |
No edit summary |
||
| Line 3: | Line 3: | ||
==SiO<sub>2</sub> Vertical Etch (Panasonic 1)== |
==SiO<sub>2</sub> Vertical Etch (Panasonic 1)== |
||
*[[media:Panasonic1-SiO-Etch.pdf|SiO<sub>2</sub> Vertical Etch Recipe]] |
*[[media:Panasonic1-SiO-Etch.pdf|SiO<sub>2</sub> Vertical Etch Recipe]] |
||
==Cr Etch (Panasonic 1)== |
|||
*[[media:CrEtch(Panasonic1).pdf|Cr Etch Recipes]] |
*[[media:CrEtch(Panasonic1).pdf|Cr Etch Recipes]] |
||
Revision as of 20:55, 18 June 2013
Back to Dry Etching Recipes.