ICP Etching Recipes: Difference between revisions
Jump to navigation
Jump to search
Content deleted Content added
| Line 52: | Line 52: | ||
===InP Etch (H<sub>2</sub> Ar)=== |
===InP Etch (H<sub>2</sub> Ar)=== |
||
*[[media:UNAXIS-VLR-InP-Etch-Ar-200C-Recipe.pdf|InP Etch Recipe (H<sub>2</sub> Ar 200C)]] |
*[[media:UNAXIS-VLR-InP-Etch-Ar-200C-Recipe.pdf|Unaxis InP Etch Recipe (H<sub>2</sub> Ar 200C) Parameters]] |
||
*[[media:17-InP%26InGaAs_etch-Cl2H2Ar-Unaxis-VLR.pdf|InP-InGaAs Etch Profile (H<sub>2</sub> Ar 200C)]] |
*[[media:17-InP%26InGaAs_etch-Cl2H2Ar-Unaxis-VLR.pdf|InP-InGaAs Etch Profile (H<sub>2</sub> Ar 200C)]] |
||
Revision as of 16:16, 23 October 2013
Back to Dry Etching Recipes.