Vacuum Deposition Recipes: Difference between revisions

From UCSB Nanofab Wiki
Jump to navigation Jump to search
Content deleted Content added
Zwarburg (talk | contribs)
Zwarburg (talk | contribs)
No edit summary
Line 1: Line 1:
This table can be used to help located the needed recipe.
⚫
{| border="1" class="collapsible collapsed wikitable" style="border: 1px solid #D0E7FF; background-color:#ffffff; text-align:center;"

⚫
{| border="1" class="collapsible wikitable" style="border: 1px solid #D0E7FF; background-color:#ffffff; text-align:center;"
|-bgcolor="#D0E7FF"
|-bgcolor="#D0E7FF"
! colspan=18 height=45 width=1575|<div style="font-size: 150%;">Vacuum Deposition Recipes</div>
! colspan=18 height=45 width=1575|<div style="font-size: 150%;">Vacuum Deposition Recipes</div>

Revision as of 18:37, 2 July 2012

This table can be used to help located the needed recipe.

Vacuum Deposition Recipes

E-Beam Evaporation Sputtering Thermal Evaporation Plasma Enhanced Chemical
Vapor Deposition (PECVD)
Atomic Layer Deposition Ion-Beam Deposition (IBD) Molecular Vapor Deposition
Material E-Beam 1 (Sharon) E-Beam 2 (Custom) E-Beam 3 (Temescal) E-Beam 4 (CHA) Sputter 1 (Custom) Sputter 2
(SFI Endeavor)
Sputter 3 Sputter 4 Sputter 5 (Lesker AXXIS) Thermal 1 Thermal 2 PECVD 1
(PlasmaTherm 790)
PECVD 2
(Advanced Vacuum)
Unaxis VLR ICP-PECVD
Ag
Al
















Al2O3
AlN
















Au
B
















Co
Cr
















Cu
Fe
















Ge
Hf
















HfO2
In
















Ir
ITO
Mo
Bn
Ni
Pd
Pt
Ru
Si
SiN
SiO2
SiOxNy
Sn
SrF2
Ta
Ta2O5
Ti
TiN
TiO2
V
W
Zn
ZnO2
Zr
ZrO2

Recipes

E-Beam Evaporation

Sputtering

Thermal Evaporation

Plasma Enhanced Chemical Vapor Deposition (PECVD)

Atomic Layer Deposition (ALD)

Ion-Beam Deposition (IBD)

==Molecular Vapor Deposition (MVD)