=[[CAIBE (Oxford Ion Mill)]]=
=[[CAIBE (Oxford Ion Mill)]]=
*[[media:42-Etching_Platinum_using_Oxford_Ion_Mill_Tool-a.pdf|Pt Etch Recipe]]
*[[media:42-Etching_Platinum_using_Oxford_Ion_Mill_Tool-a.pdf|Pt Etch Recipe]]
*[[media:|Au Etch Recipe]]
*[[media:44-Etching_Gold_with_Al2O3_Mask_using_Oxford_Ion_Mill_Tool.pdf|Au Etch Recipe]]