==ZnS Etching (RIE 2)== |
==ZnS Etching (RIE 2)== |
||
*[[media:| |
*[[media:|ZnS Etch Recipe - CH<sub>4</sub>-H<sub>2</sub>-Ar]] |
||
==ITO Etching (RIE 2)== |
==ITO Etching (RIE 2)== |
||
Revision as of 17:06, 29 July 2016
Back to Dry Etching Recipes.
RIE 1 (Custom)
RIE 2 (MRC)
CdZnTe Etching (RIE 2)
ZnS Etching (RIE 2)
- [[media:|ZnS Etch Recipe - CH4-H2-Ar]]