Template:Announcements: Difference between revisions

From UCSB Nanofab Wiki
Jump to navigation Jump to search
Content deleted Content added
m Gasonics: Up: grammar
Line 26: Line 26:


===== Gasonics: Up =====
===== Gasonics: Up =====
The process chamber mechanical pump is struggling to make base pressure but the system is able to successfully run. We are waiting for the replacement pump to repaired and returned.
The process chamber mechanical pump is struggling to make base pressure but the system is able to successfully run. We are waiting for the replacement pump to be repaired and returned.
// [[User:John d|Posted:]] 10:14, 12 February 2018 (PST)
// [[User:John d|Posted:]] 10:14, 12 February 2018 (PST)


===== Cary 500 Down =====
===== Cary 500 Down =====

Revision as of 05:44, 20 February 2018

UCSB NanoFab Announcements

Announcements

There are no general announcements at this time. // Posted: 09:58, 4 January 2018 (PST)

ICP#1: Up

He cooling fixed. // Posted: 01:32, 15 February 2018 (PST)

JEOL SEM #2: Up

System up for use. JEOL service returning on Tues for permanent fix. // Posted: 22:30, 16 February 2018 (PST)

Gasonics: Up

The process chamber mechanical pump is struggling to make base pressure but the system is able to successfully run. We are waiting for the replacement pump to be repaired and returned. // Posted: 10:14, 12 February 2018 (PST)

Cary 500 Down

UV-Vis Detector Failure. Tool is able to used from 600nm and up. Looking into replacement options. // Posted: 13:47, 12 February 2018 (PST)