===== NanoFab Shutdown 3/21 for 1.5hrs ===== |
===== NanoFab Shutdown 3/21 for 1.5hrs ===== |
||
The Nanofab will be closed Wed 3/21 from 7am-8:30am. Campus EH&S needs to replace the power supply as soon as possible as it controls other elements in the safety system for ESB. Please do not be in the lab or enter the lab between those two times. |
The Nanofab will be closed Wed 3/21 from 7am-8:30am. Campus EH&S needs to replace the power supply as soon as possible as it controls other elements in the safety system for ESB. Please do not be in the lab or enter the lab between those two times. |
||
// [[User:John d|John d]] |
// [[User:John d|John d]] 23:43, 20 March 2018 (PDT) |
||
===== Plasma-Therm DSEiii: repair in progress ===== |
===== Plasma-Therm DSEiii: repair in progress ===== |
||
Revision as of 06:43, 21 March 2018
UCSB NanoFab Announcements
NanoFab Shutdown 3/21 for 1.5hrs
The Nanofab will be closed Wed 3/21 from 7am-8:30am. Campus EH&S needs to replace the power supply as soon as possible as it controls other elements in the safety system for ESB. Please do not be in the lab or enter the lab between those two times. // John d 23:43, 20 March 2018 (PDT)
Plasma-Therm DSEiii: repair in progress
The wafer clamp cracked. Replacement is installed. Will be completed tomorrow (Wed 3/21). // Posted: 18:00, 20 March 2018 (PDT)
EBeam #4: Down for Upgrades
The upgrade is complete and working well. All users will be required to be trained again. The high voltage, sweep and turret controls are all new. Training sessions will be at 9am, 10am, 11am and 4pm Tuesday , 9am, 10am and 11am Wednesday. I will arrange other "retraining" sessions next week. // Posted: 13:57, 20 March 2018 (PDT)
PECVD #2: UP with possible High Particulates
We are still experiencing high particle counts in the Advanced Vacuum PECVD process. Our next step is to replace the Silane MFC. I will update you once I have a lead time on the new MFC. Most likely it will take several weeks to receive. Until then, the system is operational and can be used if your process is not sensitive to high particle counts. // Posted: 13:22, 19 March 2018 (PDT)
Gasonics: Up
The process chamber mechanical pump is struggling to make base pressure but the system is able to successfully run. We are waiting for the replacement pump to be repaired and returned. // Posted: 10:14, 12 February 2018 (PST)
Cary 500 Down
UV-Vis Detector Failure. Tool is able to used from 600nm and up. Looking into replacement options. // Posted: 13:47, 12 February 2018 (PST)