Wafer Bonder (Logitech WBS7): Difference between revisions

From UCSB Nanofab Wiki
Jump to navigation Jump to search
Content deleted Content added
real photo of the tool
m →About: minor formatting, added CMP mounting use
Line 11: Line 11:
== About ==
== About ==


This tool is most often used for bonding samples to Silicon carrier wafers with CrystalBond wax. This can be used for through-etching of the sample wafer, for dicing, or sometimes for lithography.
This tool is most often used for bonding samples to Silicon carrier wafers with CrystalBond wax.


This mounting method can be used for
* securing small parts for use on 100mm tools (such as the CMP)
* providing a carrier wafer for through-etching of the sample wafer
* for dicing
* for lithography
A user can place the two wafers to be bonded in contact, with the adhesive in between (such as wax, photoresist etc.). A rubber membrane is lowered on top, creating a small vacuum chamber. The tool can then be programmed to heat the wafers and melt the wax/cure the adhesive, while vacuum is pulled in the chamber, which pulls the rubber membrane down onto the top wafer. This flattens the bond and evacuates bubbles from between the wafers, providing a planar bond.
A user can place the two wafers to be bonded in contact, with the adhesive in between (such as wax, photoresist etc.). A rubber membrane is lowered on top, creating a small vacuum chamber. The tool can then be programmed to heat the wafers and melt the wax/cure the adhesive, while vacuum is pulled in the chamber, which pulls the rubber membrane down onto the top wafer. This flattens the bond and evacuates bubbles from between the wafers, providing a planar bond.


Line 18: Line 23:
==Detailed Specifications==
==Detailed Specifications==
* Substrate Size: 4"-6"
* Substrate Size: 4"-6"
* Temperature Range: 20c-188c
* Temperature Range: 20°C-188°C


==Operation Procedures==
==Operation Procedures==

Revision as of 17:11, 9 April 2019

Wafer Bonder (Logitech WBS7)
Tool Type Thermal Processing
Location Bay 5
Supervisor Don Freeborn
Supervisor Phone (805) 893-7975
Supervisor E-Mail dfreeborn@ece.ucsb.edu
Description Wafer Bonder WSB7
Manufacturer Logitech


About

This tool is most often used for bonding samples to Silicon carrier wafers with CrystalBond wax.

This mounting method can be used for

  • securing small parts for use on 100mm tools (such as the CMP)
  • providing a carrier wafer for through-etching of the sample wafer
  • for dicing
  • for lithography

A user can place the two wafers to be bonded in contact, with the adhesive in between (such as wax, photoresist etc.). A rubber membrane is lowered on top, creating a small vacuum chamber. The tool can then be programmed to heat the wafers and melt the wax/cure the adhesive, while vacuum is pulled in the chamber, which pulls the rubber membrane down onto the top wafer. This flattens the bond and evacuates bubbles from between the wafers, providing a planar bond.

We also have recipes for spin-coating the crystalbond wax, allowing for a uniform coating of the adhesive wax.

Detailed Specifications

  • Substrate Size: 4"-6"
  • Temperature Range: 20°C-188°C

Operation Procedures

Recipes