== Photoresist and ARC (RIE 5) ==
== Photoresist and ARC (RIE 5) ==


=== DUV42P (AR2) etching: ===
=== DUV42P (AR2) etching ===
* O2 = 20sccm // Pressure = 10mT // RF = 100W // Time = 40 sec
* O2 = 20sccm // Pressure = 10mT // RF = 100W // Time = 40 sec
* No need to pump/purge, can etch right away.
* No need to pump/purge, can etch right away.