Process Group - Process Control Data: Difference between revisions
Jump to navigation
Jump to search
Content deleted Content added
increased all heading levels to get HR's between Dep/Etch sections |
New Litho section + Stepper3 ASML section with links to process control data |
||
| Line 87: | Line 87: | ||
*[[Oxford ICP Etcher - Process Control Data|InP Ridge Etch with Cl2/CH4/H2 @ 60°C]] - ''No data prior to 2023-01-20'' |
*[[Oxford ICP Etcher - Process Control Data|InP Ridge Etch with Cl2/CH4/H2 @ 60°C]] - ''No data prior to 2023-01-20'' |
||
= Lithography (Process Control Data) = |
|||
''Process Control Data for Nanofab Lithography/patterning tools.'' |
|||
<hr style="height:5px"> |
|||
<hr style="height:5px"> |
|||
== Stepper #3 - ASML DUV == |
|||
*''The Process Group regularly measures data on lithography Critical Dimension ("CD") and Wafer-stage Particulate Contamination for this tool, using a sensitive lithography process that will reveal small changes in Dose repeatability and wafer flatness.'' |
|||
*[https://docs.google.com/spreadsheets/d/1xW1TFH_QjPMWl9T1jiKzwmYe4B2wg7KY-nqOKUoXttI/edit#gid=1804752281 '''Plots of CD Repeatability'''] |
|||
*[https://docs.google.com/spreadsheets/d/1xW1TFH_QjPMWl9T1jiKzwmYe4B2wg7KY-nqOKUoXttI/edit#gid=0 '''Data for CD Uniformity and Particulate Contamination'''] |
|||
Revision as of 21:04, 10 March 2023
These are the same links found on individual tool pages, in the Recipes > <<tool page>> > Process Control section.
Deposition (Process Control Data)
Process Control data for various deposition tools in the lab.
PECVD #1 (PlasmaTherm 790)
PECVD #2 (Advanced Vacuum)
ICP-PECVD (Unaxis VLR Dep)
- ICP-PECVD: Plots of SiO2 Films
- ICP-PECVD: Plots of Si3N4 Films
- ICP-PECVD: SiO2 Low-Dep Rate (LDR)
- ICP-PECVD: SiO2 High-Dep Rate (HDR)
- ICP-PECVD: Si3N4
- ICP-PECVD: Si3N4 Low-Stress
Ion Beam Sputter Deposition (Veeco Nexus)
Old Data (Pre 2022)
Old data in a different format can be found below:
Etching (Process Control Data)
Process Control data for various dry etching tools in the lab.
PlasmaTherm SLR Fluorine Etcher
- SiO2 Etching with CHF3/CF4 - Etch Data
- SiO2 Etching with CHF3/CF4 - Plots

Click for Process Control Charts
OLD Process Control Data
- SiO2 Etching with CHF3/CF4 (FL-ICP) - No data prior to 2023-01-20
Panasonic ICP #1
Old Process Control Data
- SiO2 Etch with CHF3/CF4 (Panasonic 1) - No data prior to 2023-01-20
Panasonic ICP#2
Old Process Control Data
- SiO2 Etching with CHF3/CF4 - ICP2 - No data prior to 2023-01-20
Unaxis VLR Etch
Oxford PlasmaPro Cobra Etcher
Calibration / Process testing data taken using the "InP Ridge Etch" process: Cl2/CH4/H2 @ 60°C, 1cm piece with ~50% SiO2 hardmask.
- "Std InP Ridge Etch" Cl2/CH4/H2/60°C - Etch Data Tables
- "Std InP Ridge Etch" Cl2/CH4/H2/60°C - Plots

Click for Process Control Charts
Old Process Control Data
- InP Ridge Etch with Cl2/CH4/H2 @ 60°C - No data prior to 2023-01-20
Lithography (Process Control Data)
Process Control Data for Nanofab Lithography/patterning tools.
Stepper #3 - ASML DUV
- The Process Group regularly measures data on lithography Critical Dimension ("CD") and Wafer-stage Particulate Contamination for this tool, using a sensitive lithography process that will reveal small changes in Dose repeatability and wafer flatness.
- Plots of CD Repeatability
- Data for CD Uniformity and Particulate Contamination