|{{rl|ICP Etching Recipes|GaAs-AlGaAs Etch (Panasonic 1)}} |
|{{rl|ICP Etching Recipes|GaAs-AlGaAs Etch (Panasonic 1)}} |
||
| |
| |
||
|[[ICP Etching Recipes#GaAs Etch .28Oxford ICP Etcher.29|R]] |
|||
|R2 |
|||
|{{rl|ICP Etching Recipes|ICP-Etch (Unaxis VLR)|GaAs-AlGaAs Etch (Unaxis VLR)|AlGaAs Etch (Unaxis VLR)}} |
|{{rl|ICP Etching Recipes|ICP-Etch (Unaxis VLR)|GaAs-AlGaAs Etch (Unaxis VLR)|AlGaAs Etch (Unaxis VLR)}} |
||
| |
| |
||
| Line 364: | Line 364: | ||
| |
| |
||
| |
| |
||
|[[ICP Etching Recipes#GaN Etch .28Oxford ICP Etcher.29|R]] |
|||
|R1 |
|||
|{{rl|ICP Etching Recipes|GaN Etch (Unaxis VLR)}} |
|{{rl|ICP Etching Recipes|GaN Etch (Unaxis VLR)}} |
||
| |
| |
||
| Line 436: | Line 436: | ||
|{{rl|ICP Etching Recipes|GaAs-AlGaAs Etch (Panasonic 1)}} |
|{{rl|ICP Etching Recipes|GaAs-AlGaAs Etch (Panasonic 1)}} |
||
|{{rl|ICP Etching Recipes|GaAs Etch (Panasonic 2)}} |
|{{rl|ICP Etching Recipes|GaAs Etch (Panasonic 2)}} |
||
|[[ICP Etching Recipes#GaAs Etch .28Oxford ICP Etcher.29|R]] |
|||
|R3 |
|||
|{{rl|ICP Etching Recipes|ICP-Etch (Unaxis VLR)|GaAs-AlGaAs Etch (Unaxis VLR)|GaAs Etch (Unaxis VLR)}} |
|{{rl|ICP Etching Recipes|ICP-Etch (Unaxis VLR)|GaAs-AlGaAs Etch (Unaxis VLR)|GaAs Etch (Unaxis VLR)}} |
||
| |
| |
||
| Line 454: | Line 454: | ||
|{{rl|ICP Etching Recipes|GaN Etch (Panasonic 1)}} |
|{{rl|ICP Etching Recipes|GaN Etch (Panasonic 1)}} |
||
|A |
|A |
||
|[[ICP Etching Recipes#GaN Etch .28Oxford ICP Etcher.29|R]] |
|||
|R3 |
|||
|{{rl|ICP Etching Recipes|GaN Etch (Unaxis VLR)}} |
|{{rl|ICP Etching Recipes|GaN Etch (Unaxis VLR)}} |
||
| |
| |
||
| Line 526: | Line 526: | ||
| |
| |
||
| |
| |
||
|[[ICP Etching Recipes#InP Ridge Etch .28Oxford ICP Etcher.29|R]] |
|||
|R3 |
|||
|{{rl|ICP Etching Recipes|ICP-Etch (Unaxis VLR)|InP-InGaAs-InAlAs Etch (Unaxis VLR)|InP Etch (Unaxis VLR)}} |
|{{rl|ICP Etching Recipes|ICP-Etch (Unaxis VLR)|InP-InGaAs-InAlAs Etch (Unaxis VLR)|InP Etch (Unaxis VLR)}} |
||
| |
| |
||
| Line 544: | Line 544: | ||
|A |
|A |
||
|A |
|A |
||
|[[ICP Etching Recipes#InP Ridge Etch .28Oxford ICP Etcher.29|R]] |
|||
|R6 |
|||
|{{rl|ICP Etching Recipes|ICP-Etch (Unaxis VLR)|InP-InGaAs-InAlAs Etch (Unaxis VLR)|InP Etch (Unaxis VLR)}} |
|{{rl|ICP Etching Recipes|ICP-Etch (Unaxis VLR)|InP-InGaAs-InAlAs Etch (Unaxis VLR)|InP Etch (Unaxis VLR)}} |
||
| |
| |
||
Revision as of 21:15, 26 July 2024
Process Control Data
See above linked page for process control data (dep rate/stress etc. over time), for a selection of often-used dry etches
Dry Etching Tools/Materials Table
The Key/Legend for this table's A...R5 values is at the bottom of the page.
Process Ranking Table
Processes in the table above are ranked by their "Process Maturity Level" as follows:
| Process Level | Description of Process Level Ranking | ||||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|
| A | Process Allowed and materials available but never done | ||||||||||
| R1 | Process has been run at least once | ||||||||||
| R2 | Process has been run and/or procedure is documented or/and data available | ||||||||||
| R3 | Process has been run, procedure is documented, and data is available | ||||||||||
| R4 | Process has a documented procedure with regular (≥4x per year) data or lookahead/in-situ control available | ||||||||||
| R5 | Process has a documented procedure with regular (≥4x per year) data and lookahead/in-situ control available | ||||||||||
| R6 | Process has a documented procedure, regular ( ≥4x per year) data, and control charts & limits available | ||||||||||