Process Group - Process Control Data: Difference between revisions
(linked to EB-eam #1 sheets - plots not ready yet) |
(→Deposition, Metal (Process Control Data): added all eBeam 1 data + plots) |
||
Line 76: | Line 76: | ||
=== E-Beam 1: Ti === |
=== E-Beam 1: Ti === |
||
*[https://docs.google.com/spreadsheets/d/ |
*[https://docs.google.com/spreadsheets/d/1biiHilf-DZhizDz2tMp6z7nQBeOYA6r8gnqA1WEHB5A/edit?gid=0#gid=0 Titanium Datasheet] |
||
*[https://docs.google.com/spreadsheets/d/1biiHilf-DZhizDz2tMp6z7nQBeOYA6r8gnqA1WEHB5A/edit?gid=1305007052#gid=1305007052 Titanium Plots] |
|||
*Titanium Plots - ''To Be Added'' |
|||
=== E-Beam 1: Au === |
=== E-Beam 1: Au === |
||
*[https://docs.google.com/spreadsheets/d/ |
*[https://docs.google.com/spreadsheets/d/1biiHilf-DZhizDz2tMp6z7nQBeOYA6r8gnqA1WEHB5A/edit?gid=1762267354#gid=1762267354 Gold Datasheet] |
||
*[https://docs.google.com/spreadsheets/d/1biiHilf-DZhizDz2tMp6z7nQBeOYA6r8gnqA1WEHB5A/edit?gid=1245613525#gid=1245613525 Gold Plots] |
|||
*Gold Plots - ''To Be Added'' |
|||
=== E-Beam 1: Cr === |
=== E-Beam 1: Cr === |
||
*[https:// |
*[https://wiki.nanofab.ucsb.edu/wiki/Process_Group_-_Process_Control_Data?veaction=edit§ion=7 Chromium Datasheet] |
||
*[https://docs.google.com/spreadsheets/d/1biiHilf-DZhizDz2tMp6z7nQBeOYA6r8gnqA1WEHB5A/edit?gid=424169133#gid=424169133 Chromium Plots] |
|||
*Chromium Plots - ''To Be Added'' |
|||
=== E-Beam 1: Ni === |
=== E-Beam 1: Ni === |
||
*[https://docs.google.com/spreadsheets/d/ |
*[https://docs.google.com/spreadsheets/d/1biiHilf-DZhizDz2tMp6z7nQBeOYA6r8gnqA1WEHB5A/edit?gid=679240351#gid=679240351 Nickel Datasheet] |
||
*[https://docs.google.com/spreadsheets/d/1biiHilf-DZhizDz2tMp6z7nQBeOYA6r8gnqA1WEHB5A/edit?gid=1463522927#gid=1463522927 Nickel Plots] |
|||
*Nickel Plots - ''To Be Added'' |
|||
<hr style="height:5px"> |
<hr style="height:5px"> |
Revision as of 18:29, 21 May 2025
Process Control Data are standardized processes, run by the NanoFab, allowing for day-to-day or year-by-year comparisons of a tool's performance at the process level. This is similar Statistical Process Control (SPC).
These are the same links are found on individual tool pages, in the <<tool page>> > Process Control section.
Data are collected by our Process Group Interns and reviewed by Process Group Staff.
Deposition, Dielectric (Process Control Data)
Process Control data for various deposition tools in the lab.
PECVD #1 (PlasmaTherm 790)
PECVD #2 (Advanced Vacuum)
ICP-PECVD (Unaxis VLR Dep)
- ICP-PECVD: Plots of SiO2 Films
- ICP-PECVD: Plots of Si3N4 Films
- ICP-PECVD: SiO2 Low-Dep Rate (LDR)
- ICP-PECVD: SiO2 High-Dep Rate (HDR)
- ICP-PECVD: Si3N4
- ICP-PECVD: Si3N4 Low-Stress
Ion Beam Sputter Deposition (Veeco Nexus)
Old Data (Pre 2022)
Old data in a different format can be found below:
Deposition, Metal (Process Control Data)
Process Control data for various Metal evaporators in the lab.
E-Beam 4 (CHA)
E-Beam 4: Ti
E-Beam 4: Au
E-Beam 4: Cr
E-Beam 4: Ni
E-Beam 1 (Sharon)
E-Beam 1: Ti
E-Beam 1: Au
E-Beam 1: Cr
E-Beam 1: Ni
Etching (Process Control Data)
Process Control data for various dry etching tools in the lab.
PlasmaTherm SLR Fluorine Etcher
SiO2 Etching (FL-ICP Process Control)
We have found that SiO2 etching is fairly insensitive to chamber condition.
Old SiO2 Process Control Data
- SiO2 Etching with CHF3/CF4 (FL-ICP) - No data prior to 2023-01-20
Si Etching (FL-ICP Process Control)
This Si etch is much more sensitive to chamber condition, allowing us to detect chamber contamination faster.
- Recipe: SiVertHFv2 - C4F8/SF6/CF4 etch of 100mm Silicon Wafer with ~50% open area and resist mask
Panasonic ICP #1
Old Process Control Data
- SiO2 Etch with CHF3/CF4 (Panasonic 1) - No data prior to 2023-01-20
Panasonic ICP#2
Old Process Control Data
- SiO2 Etching with CHF3/CF4 - ICP2 - No data prior to 2023-01-20
Unaxis VLR Etch
Oxford PlasmaPro Cobra Etcher
InP Ridge Etch: Cl2/CH4/H2/60°C
Calibration / Process testing data taken using the "InP Ridge Etch" process: Cl2/CH4/H2 @ 60°C, 1cm piece with ~50% SiO2 hardmask.
- "Std InP Ridge Etch" Cl2/CH4/H2/60°C - Etch Data Tables
- "Std InP Ridge Etch" Cl2/CH4/H2/60°C - Plots
Old InP Ridge Etch Data
- InP Ridge Etch with Cl2/CH4/H2 @ 60°C - No data prior to 2023-01-20
GaN Etch (Cl2/BCl3/Ar/200°C)
Recipe: Std GaN Etch - BCl3/Cl2/Ar - 200C (Public), on 1cm x 1cm ~1.2µm deep GaN etch with Cl2/BCl3/Ar at 200°C. Sapphire substrate with SiO2 mask for GaN.
PlasmaTherm DSEIII Deep Silicon Etcher
Si Bosch Etching C4F8/SF6/Ar
- Recipe: STD_Bosch_Si (⭐️Production), on 100mm Si Wafer with ~50% open area, photoresist mask, ~40µm deep
Lithography (Process Control Data)
Process Control Data for Nanofab Lithography/patterning tools.
Stepper #3 (ASML DUV)
- The Process Group regularly measures data on lithography Critical Dimension ("CD") and Wafer-stage Particulate Contamination for this tool, using a sensitive lithography process that will reveal small changes in Dose repeatability and wafer flatness.
- Plots of CD Repeatability
- Data for CD Uniformity and Particulate Contamination
- Example of Data Table with SEM's of 320nm features. Click for full data table.Example SPC Chart - Measured Critical Dimension "CD" versus Date. Click for charts.