Lithography Recipes: Difference between revisions

From UCSB Nanofab Wiki
Jump to navigation Jump to search
Content deleted Content added
No edit summary
No edit summary
Line 25: Line 25:
*{{fl|AZnLOF2020-Negative-Resist-Datasheet.pdf|AZnLOF2000 (AZnLOF2020, AZnLOF2035, AZnLOF2070)}}
*{{fl|AZnLOF2020-Negative-Resist-Datasheet.pdf|AZnLOF2000 (AZnLOF2020, AZnLOF2035, AZnLOF2070)}}
*{{fl|UVN2300-Negative-Resist-Datasheet.pdf|UVN2300-0.5}}
*{{fl|UVN2300-Negative-Resist-Datasheet.pdf|UVN2300-0.5}}
*{{fl|xxxx.pdf|SU-8-2015 and 2075}}


;Underlayers
;Underlayers
Line 36: Line 37:
*{{fl|maN2403-E-Beam-Resist-Datasheet.pdf|maN 2403}}
*{{fl|maN2403-E-Beam-Resist-Datasheet.pdf|maN 2403}}


⚫
|
;Nanoimprinting
;Nanoimprinting


*{{fl|NX1020-Nanoimprinting-Datasheet.pdf|NX1020}}
*{{fl|NX1020-Nanoimprinting-Datasheet.pdf|NX1020}}
*{{fl|MRI-7020-Nanoimprinting-Datasheet.pdf|MRI-7020}}
*{{fl|MRI-7020-Nanoimprinting-Datasheet.pdf|MRI-7020}}
⚫
|

;Contrast Enhancement Materials
;Contrast Enhancement Materials


Line 51: Line 51:
*{{fl|AR2-Anti-Reflective-Coating.pdf|AR2}}
*{{fl|AR2-Anti-Reflective-Coating.pdf|AR2}}
*{{fl|DS-K101-Anti-Reflective-Coating.pdf|DS-K101 (developable BARC)}}
*{{fl|DS-K101-Anti-Reflective-Coating.pdf|DS-K101 (developable BARC)}}

;Adhesion Promoters

*{{fl|xxxx.pdf|HMDS}}
*{{fl|xxxx.pdf|AP3000 BCB Adhesion Promoter}}
*{{fl|xxxx.pdf|Omnicoat, SU-8 Adhesion Promoter}}

;BCB and SOG

*{{fl|xxxx.pdf|BCB, Cyclotene 3022-46(Not Photosensitive)}}
*{{fl|xxxx.pdf|PhotoBCB, Cyclotene 4022-40(Negative Polarity)}}
*{{fl|xxxx.pdf|Spin-on-Glass, Honeywell 512B (Not Photosensitive)}}


;Developers
;Developers
Line 56: Line 68:
*{{fl|AZ400K-Developer-Datasheet.pdf|AZ400K (AZ400K, AZ400K1:4)}}
*{{fl|AZ400K-Developer-Datasheet.pdf|AZ400K (AZ400K, AZ400K1:4)}}
*{{fl|AZ300MIF-Developer-Datasheet.pdf|AZ300MIF}}
*{{fl|AZ300MIF-Developer-Datasheet.pdf|AZ300MIF}}
*{{fl|xxxxxx.pdf|DS2100 BCB Developer}}
*{{fl|xxxxxx.pdf|SU-8 Developer}}
*{{fl|xxxxxx.pdf|101A Developer (for DUV Flood Exposed PMGI)}}


;Photoresist Removers
;Photoresist Removers
Line 62: Line 77:
*{{fl|AZ300T-Resist-Remover.pdf|AZ300T}}
*{{fl|AZ300T-Resist-Remover.pdf|AZ300T}}
*{{fl|PRX-127-Resist-Remover.pdf|PRX-127}}
*{{fl|PRX-127-Resist-Remover.pdf|PRX-127}}
*{{fl|xxxx.pdf|Remover PG, SU-8 stripper}}


|}
|}

Revision as of 23:33, 10 July 2013

Lift-Off Techniques

Chemical Datasheets

Positive Photoresists
Negative Photoresists
Underlayers
E-beam resists
Nanoimprinting
Contrast Enhancement Materials
Anti-Reflection Coatings
Adhesion Promoters
BCB and SOG
Developers
Photoresist Removers

Recipes

  • R = Recipe is available. Clicking this link will take you to the recipe.
  • A = Material is available for use, but no recipes are provided.


Lithography Recipes

Contact Aligners Steppers Flood Expose E-Beam Lithography
Positive Resists SUSS MJB-3 SUSS MA-6 Stepper 1
(GCA 6300)
Stepper 2
(AutoStep 200)
Stepper 3
(ASML DUV)
MLA150
(Heidelberg)


AZ4110 R1 R1 A A
AZ4210 R1 R1 A A



AZ4330RS R1 R1 A A
OCG 825-35CS A A A A



SPR 950-0.8 A A A A
SPR 955 CM-0.9 A A R1 R1



SPR 955 CM-1.8 A A R1 R1
SPR 220-3.0 R1 R1 R1 R1



SPR 220-7.0 R1 R1 R1 R1
THMR-IP3600 HP D

A A



UV6-0.7 R1
UV210-0.3 R1
Negative Resists SUSS MJB-3 SUSS MA-6 Stepper 1
(GCA 6300)
Stepper 2
(AutoStep 200)
Stepper 3
(ASML DUV)
MLA150
(Heidelberg)


AZ5214-EIR R1 R1 R1 R1
AZnLOF 2020 R1 R1 R1 R1
AZnLOF 2035 A A A A
AZnLOF 2070 A A A A
AZnLOF 5510 A A R1 R1
UVN2300-0.5 R1
SU-8 2015 A A A A
Underlayers SUSS MJB-3 SUSS MA-6 Stepper 1
(GCA 6300)
Stepper 2
(AutoStep 200)
Stepper 3
(ASML DUV)
MLA150
(Heidelberg)


PMGI SF-11







PMGI SF-15
LOL 2000
XHRIC-11 (i-lineBARC)
AR-2 (DUV BARC)
DS-K101 (DUV BARC)
Overlayers SUSS MJB-3 SUSS MA-6 Stepper 1
(GCA 6300)
Stepper 2
(AutoStep 200)
Stepper 3
(ASML DUV)
MLA150
(Heidelberg)


CEM-365 IS
E-Beam Resists SUSS MJB-3 SUSS MA-6 Stepper 1
(GCA 6300)
Stepper 2
(AutoStep 200)
Stepper 3
(ASML DUV)
MLA150
(Heidelberg)


 ??????
 ???????
Nanoimprint Resists SUSS MJB-3 SUSS MA-6 Stepper 1
(GCA 6300)
Stepper 2
(AutoStep 200)
Stepper 3
(ASML DUV)
MLA150
(Heidelberg)


MR-I 7020
Nanonex NX-1020
SUSS MJB-3 SUSS MA-6 Stepper 1
(GCA 6300)
Stepper 2
(AutoStep 200)
Stepper 3
(ASML DUV)
MLA150
(Heidelberg)