The high-energy sputter deposition produces denser films than other techniques, improving optical damage threshold (and thus coating lifetime). This also causes the refractive indices to be slightly higher than comparable stoichiometric films deposited by other techniques.
The high-energy sputter deposition produces denser films than other techniques, improving optical damage threshold (and thus coating lifetime). This also causes the refractive indices to be slightly higher than comparable stoichiometric films deposited by other techniques.


Four metallic targets can be installed. Currently available targets are Ta, Si, Al, Ti & ITO (producing Oxides & Nitrides of each). Ta & Si are always available, the others are rotated out as users need.
Four metallic targets can be installed. Currently available targets are '''Ta, Si, Al, Ti & ITO''' (producing Oxides & Nitrides of each). Ta & Si are always available, the others are rotated out as users need.


The most common films for High-/Anti-Reflection (HR/AR) coatings are SiO<sub>2</sub> & Ta<sub>2</sub>O<sub>5</sub>, both of which are extremely stable w/r/to refractive index. Users typically calibrate their dep. rates prior to critical deps. & multi-layer coatings.
The most common films for High-/Anti-Reflection (HR/AR) coatings are '''SiO<sub>2</sub>''' & '''Ta<sub>2</sub>O<sub>5</sub>''', both of which are extremely stable w/r/to refractive index. Users typically calibrate their dep. rates prior to critical deps. & multi-layer coatings.


= Detailed Specifications =
= Detailed Specifications =

Revision as of 19:54, 13 August 2013

Ion Beam Deposition (Veeco NEXUS)
Tool Type Vacuum Deposition
Location Bay 3
Supervisor Mike Silva
Supervisor Phone (805) 893-3096
Supervisor E-Mail silva@ece.ucsb.edu
Description Ion Beam Deposition Tool
Manufacturer Veeco
Vacuum Deposition Recipes
Sign up for this tool


About

This tool is designed for high quality, precise, reproducible deposition of dielectric films for optical quality films. Metallic material is ion bombarded from a target material and a reactive ion beam of oxygen and/or nitrogen is aimed at the surface, creating a metal-oxide or nitride on the sample. The system is fully computer controlled to facilitate multi-layer stack recipes for high reflectivity or low reflectivity coatings. The system is load locked and can handle wafers up to 6” in diameter as well as small pieces. Sample rotation and angling is used to facilitate material quality and allows for sidewall coverage on non-planar surfaces. Uniformity is better than 1.5% over 6" wafers and reproducibility is expected to be within one percent (with pre-dep calibration). The high-energy sputter deposition produces denser films than other techniques, improving optical damage threshold (and thus coating lifetime). This also causes the refractive indices to be slightly higher than comparable stoichiometric films deposited by other techniques.

Four metallic targets can be installed. Currently available targets are Ta, Si, Al, Ti & ITO (producing Oxides & Nitrides of each). Ta & Si are always available, the others are rotated out as users need.

The most common films for High-/Anti-Reflection (HR/AR) coatings are SiO2 & Ta2O5, both of which are extremely stable w/r/to refractive index. Users typically calibrate their dep. rates prior to critical deps. & multi-layer coatings.

Detailed Specifications

  • Xenon target bombardment
  • Nitrogen and/or Oxygen deposition assist source for metal oxides/nitrides
  • Ta and Si targets (Al and Ti coming soon)
  • Pieces up to 6” wafers accepted
  • Full programmable control through GUI for multi-layer optical coatings
  • Ta2O5 (1.33 A/s rate) and SiO2 (0.85A/s)characterized, standard recipes
  • Base Pressure ~ 3e-8 Torr
  • High quality, high reflectivity (>99.5%) mirrors demonstrated in blue wavelengths