=[[ICP Etch 1 (Panasonic E626I)]]= |
=[[ICP Etch 1 (Panasonic E626I)]]= |
||
==SiO<sub>2</sub> Etching (Panasonic 1)== |
==SiO<sub>2</sub> Etching (Panasonic 1)== |
||
*[[media:Panasonic1-SiO-Etch.pdf|SiO<sub>2</sub> Vertical Etch Recipe]] |
*[[media:Panasonic1-SiO-Etch.pdf|SiO<sub>2</sub> Vertical Etch Recipe Parameters]] |
||
*[[media:Panasonic1-SiO2-Data-Process-Variation-CHF3-revA.pdf|SiO<sub>2</sub> CHF3 Etch Variations]] |
*[[media:Panasonic1-SiO2-Data-Process-Variation-CHF3-revA.pdf|SiO<sub>2</sub> CHF3 Etch Variations]] |
||