UCSB NanoFab Announcements

Ebeam#2: heater repair scheduled

We will be performing heater repair on Monday Aug. 18th. System should be ready for use Tuesday. // John d 11:28, 18 August 2018 (PDT)

PECVD#1: Software Upgrade

Plasmatherm will be upgrading the system software on September 17th. The upgrade will take 3-5 days. After the upgrade is complete, everyone must be re-certified to use the tool. Please document any custom recipes that you may have, in case they can't be copied over. // John d 06:38, 15 August 2018 (PDT)

RIE#5: SiCl4 Issue

We have a flow rate problem on the SiCl4 gas line. You can only flow the SiCl4 for 5 minutes and then you have to wait 5 minutes before you flow it again. So in order to to do a 10 minute Etch you will have to do it in three steps flow 5 mi, wait 5mi, then flow 5min. // John d 17:22, 15 June 2018 (PDT)