Oxford ICP Etcher (PlasmaPro 100 Cobra)

From UCSB Nanofab Wiki
Revision as of 20:38, 3 September 2021 by John d (talk | contribs) (first attempt at page)
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)
Jump to navigation Jump to search
Oxford ICP Etcher (PlasmaPro 100 Cobra)
Tool Type Dry Etch
Location Bay 2
Supervisor Tony Bosch
Supervisor Phone (805) 893-3486
Supervisor E-Mail bosch@ece.ucsb.edu
Description ICP Etches for III-V/ALE
Manufacturer Oxford Instruments
Model PlasmaPro 100 Cobra 300
Materials InP, GaAs, GaN, Silicon ALE
Dry Etch Recipes


About

The Oxford PlasmaPro 100 Cobra 300 is intended for etching InP-based, GaAs-baased and GaN-based epitaxies, in addition to Atomic Layer Etching (ALE) processes. The system has a load lock, wide temperature range with rapid heating/cooling, Inductively Coupled Plasma (ICP) coil and a capactively coupled substrate HF (13.56MHz) The fixturing is configured for 4" diameter Si wafers and uses a clamp to hold the sample on the RF chuck. Small pieces may be placed on Silicon carrier wafers, with or without mounting adhesive. Helium back-side cooling is used to keep the sample cool during the etch, but pieces do heat up when placed on carriers.

The in-situ laser monitor installed on this system allows for repeatable etches and endpoint detection via continuous optical monitoring of the wafer reflectivity in a user-determined location, through a porthole on the chamber. The system also has an in situ optical emission monitor for plasma spectroscopy, utilized for chamber clean endpoint detection.

Detailed Specifications

  • ICP Power: ??? W
  • RF Power: ??? W
  • Temperature Rnage: –40°C to +400°C
  • Gases Available: ** CH4, H2, Ar, Cl2, BCl3, SF6, SiCl4, O2, N2
  • He-back-side cooling
  • 100mm wafer held down with ceramic clamp., single-load
    • Users may place pieces onto carrier wafer with or without adhesive. Standard recipes use no adhesive.
    • Pieces must be >7mm from edge of carrier to avoid wafer-clamping mechanism.
  • Windows-based Cortex software control of process and wafer handling
  • Allowed Materials:
    • InP-based epitaxies
    • GaAs-baased epitaxies
    • GaN-based epitaxies
    • Silicon only for ALE (no deep etching)
  • Standard masking materials include:
    • SiO2
    • Si3N4
    • photoresist (at << 100°C).

Other materials can be exposed to the chamber only with staff approval.