Plasma Activation (EVG 810)

From UCSB Nanofab Wiki
Revision as of 19:06, 15 September 2022 by Sawyer l (talk | contribs) (Updated SOP)
Jump to navigation Jump to search
Plasma Activation (EVG 810)
Location Bay 7
Tool Type Dry Etch
Manufacturer EVG Group
Description Plasma Surface Activation

Primary Supervisor Lee Sawyer
(805) 893-2123
lee_sawyer@ucsb.edu

Secondary Supervisor

Aidan Hopkins


Recipes Dry Etch Recipes

SignupMonkey: Sign up for this tool


About

This a capacitively coupled Oxygen plasma activation system used exclusively for the surface activation of clean surfaces prior to wafer bonding. This technique allows bonding temperatures to be lowered and is used as a companion tool to the Karl-Suss SB6 wafer bond tool.

Detailed Specifications

  • Gases used: O2 and N2
  • Sample size: pieces to 6” wafer
  • Recipes characterized for substrate thicknesses between 250um and 750um. Thicknesses outside of this range need to have parameters optimized to minimize reflective power.

Documentation

Recipes

Please see the Oxygen Plasma Recipe page for standard EVG recipes.