Automated Coat/Develop System (S-Cubed Flexi)

From UCSB Nanofab Wiki
Revision as of 18:03, 3 September 2024 by John d (talk | contribs) (→Detailed Specifications: linked to PR's,)
Jump to navigation Jump to search
Automated Coat/Develop System (S-Cubed Flexi)
Location Bay 7
Tool Type Wet Processing
Manufacturer S-Cubed
Model Flexi (Custom)
Description Automatic Coat/Bake/Develop

Primary Supervisor Tony Bosch
(805) 893-3486
bosch@ece.ucsb.edu

Secondary Supervisor

Lee Sawyer


Recipes Wet Processing Recipes

SignupMonkey: Sign up for this tool


This Tool is now available for training - please contact the supervisor. 2022-11-01

About

The S3-Coater is a Coater/Developer system that has one photoresist spinner, one developer spinner and 4 hotplates each with independent temperature control and a chill plate. A central robot picks your wafer/s from one of 2 cassettes, processes them and returns them to the cassette. The system is recipe driven with a high degree of process control and minimal backside contamination, and coats photoresists with low particle counts/streaks and high uniformity.

Only full size 4-inch (100mm) substrates are allowed on this system.

Detailed Specifications

  • Wafer Size: 100mm
  • PR Coating Properties:
    • Uniformity < 1.0%
    • < 100 particles on 100mm wafer
  • Photoresists/Underlayers Available:
    • UV6-0.8 - DUV Positive imaging resist
    • DS-K101-304 - DUV bottom anti-reflection layer (BARC).
    • PMMA - NOT FOR PUBLIC USE AT THIS TIME
    • PMGI SF11 - NOT FOR PUBLIC USE AT THIS TIME
    • PMGI SF5 - NOT FOR PUBLIC USE AT THIS TIME
  • Solvents Available:
    • EBR100 (wafer backside cleaning)
  • Developers Available:
  • Hotplates Available:
    • 135°C - for UV6 soft-bake and Post-Exposure Bake
    • 220°C - for DSK101 BARC soft-bake - dry etchable
    • 185*C - for DSK101 BARC soft-bake - developable for undercut

Process Information

Operating Procedures

Recipes

  • Recipes > Lithography > Automated Coater Recipes - See all available spin-coat recipes for this machine. Only Staff may edit/create recipes.