- (download) Oxford Etcher - InP Ridge Etch using Oxford PlasmaPro 100 Cobra - 2021-09-08.pdf . . 0 × 0 . . 1.46 MB . . John d . . 01:43, 6 March 2024
- (download) Oxford Ion Mill SOP.pdf . . 0 × 0 . . 196 KB . . Millerski w . . 17:35, 13 November 2023
- (download) PC3-1500SpinOnGlassMSDS.pdf . . 0 × 0 . . 37 KB . . Zwarburg . . 19:55, 30 June 2012
- (download) PECVD1-LS SIN recipe 2014.pdf . . 0 × 0 . . 1.03 MB . . Biljana . . 23:37, 5 December 2014
- (download) PECVD1-LS SION-recipe2014 LS SION recipe.pdf . . 0 × 0 . . 1.24 MB . . Biljana . . 19:18, 10 December 2014
- (download) PECVD1-LS SION recipe 2014.pdf . . 0 × 0 . . 1.24 MB . . Biljana . . 23:23, 3 December 2014
- (download) PECVD1-PECVD SIN data-February 2014 SiN Index,dep.rates,stress.pdf . . 0 × 0 . . 106 KB . . Biljana . . 23:53, 12 March 2014
- (download) PECVD1-SiN-1000A Standard recipe.pdf . . 0 × 0 . . 296 KB . . Biljana . . 22:39, 20 March 2014
- (download) PECVD1-SiN-Data.pdf . . 0 × 0 . . 34 KB . . Zwarburg . . 19:05, 16 August 2012
- (download) PECVD1-SiN-Recipe.pdf . . 0 × 0 . . 35 KB . . Zwarburg . . 19:01, 16 August 2012
- (download) PECVD1-SiN-standard recipe.pdf . . 0 × 0 . . 189 KB . . Biljana . . 21:43, 19 March 2014
- (download) PECVD1-SiN-standard recipe 1000A.pdf . . 0 × 0 . . 295 KB . . Biljana . . 19:08, 20 March 2014
- (download) PECVD1-SiN-standard recipe 2014.pdf . . 0 × 0 . . 298 KB . . Biljana . . 21:58, 15 April 2014
- (download) PECVD1-SiN-standard recipe 2014 SiN standard recipe.pdf . . 0 × 0 . . 298 KB . . Biljana . . 17:25, 10 December 2014
- (download) PECVD1-SiN Calibration-February 2014.pdf . . 0 × 0 . . 105 KB . . Biljana . . 17:00, 13 March 2014
- (download) PECVD1-SiN Calibration-February 2014 SiN 1000A.pdf . . 0 × 0 . . 103 KB . . Biljana . . 17:07, 13 March 2014
- (download) PECVD1-SiN Data-March 2014.pdf . . 0 × 0 . . 101 KB . . Biljana . . 21:55, 19 March 2014
- (download) PECVD1-SiN data.pdf . . 0 × 0 . . 106 KB . . Biljana . . 16:37, 13 March 2014
- (download) PECVD1-SiN standard recipe 2014.pdf . . 0 × 0 . . 299 KB . . Biljana . . 17:32, 10 December 2014
- (download) PECVD1-SiO2-Data.pdf . . 0 × 0 . . 35 KB . . Zwarburg . . 19:05, 16 August 2012
- (download) PECVD1-SiO2-Recipe.pdf . . 0 × 0 . . 36 KB . . Zwarburg . . 19:03, 16 August 2012
- (download) PECVD1-SiO2-standard recipe 1000A.pdf . . 0 × 0 . . 1,007 KB . . Biljana . . 23:34, 21 March 2014
- (download) PECVD1-SiO2-standard recipe 2014.pdf . . 0 × 0 . . 299 KB . . Biljana . . 22:42, 15 April 2014
- (download) PECVD1-SiO2-standard recipe 2014 SiO2 standard recipe.pdf . . 0 × 0 . . 299 KB . . Biljana . . 18:22, 10 December 2014
- (download) PECVD1-SiON-recipe 2014 LS SION recipe.pdf . . 0 × 0 . . 1.24 MB . . Biljana . . 17:53, 1 October 2014
- (download) PECVD1-SiON-recipe 2014 LS SION recipe LS SION recipe.pdf . . 0 × 0 . . 1.24 MB . . Biljana . . 22:24, 10 October 2014
- (download) PECVD1-WIKI PECVD SiN Index, dep.rates, stress.pdf . . 0 × 0 . . 130 KB . . Biljana . . 16:55, 11 September 2013
- (download) PECVD1- SiO2 Calibratiion February 2014-1 SiO2 1000A.pdf . . 0 × 0 . . 113 KB . . Biljana . . 19:06, 13 March 2014
- (download) PECVD1- SiO2 Calibratiion February 2014 SiO2 1000A.pdf . . 0 × 0 . . 112 KB . . Biljana . . 18:20, 13 March 2014
- (download) PECVD1 Operating Instructions.pdf . . 0 × 0 . . 64 KB . . Biljana . . 20:46, 20 March 2014
- (download) PECVD1 SIN 2-pt Thickness-index uniformity March 2014.pdf . . 0 × 0 . . 82 KB . . Biljana . . 21:02, 20 March 2014
- (download) PECVD1 SIN 2-pt Thickness uniformity March 2014.pdf . . 0 × 0 . . 62 KB . . Biljana . . 23:59, 20 March 2014
- (download) PECVD1 SIN Data-April 2014 SIN data.pdf . . 0 × 0 . . 117 KB . . Biljana . . 22:29, 15 April 2014
- (download) PECVD1 SIN Data-March 2014 SIN data.pdf . . 0 × 0 . . 117 KB . . Biljana . . 22:35, 20 March 2014
- (download) PECVD1 SIN Thickness &index uniformity March 2014.pdf . . 0 × 0 . . 103 KB . . Biljana . . 21:05, 20 March 2014
- (download) PECVD1 SIN Thickness and index uniformity March 2014.pdf . . 0 × 0 . . 94 KB . . Biljana . . 21:12, 20 March 2014
- (download) PECVD1 SOP 8-26-26.pdf . . 0 × 0 . . 5.61 MB . . Barreraz . . 17:32, 1 September 2026
- (download) PECVD1 SiN data-February 2014 AFM roughness.pdf . . 0 × 0 . . 156 KB . . Biljana . . 00:09, 13 March 2014
- (download) PECVD1 SiO2 Data-April 2014 SiO2 Data.pdf . . 0 × 0 . . 116 KB . . Biljana . . 22:44, 15 April 2014
- (download) PECVD1 SiO2 Data-March 2014 SiO2 Data.pdf . . 0 × 0 . . 116 KB . . Biljana . . 19:06, 21 March 2014
- (download) PECVD2-SiN-Data.pdf . . 0 × 0 . . 36 KB . . Zwarburg . . 19:07, 16 August 2012
- (download) PECVD2-SiN-Recipe-100SiH4-100C-Low-Stress.pdf . . 0 × 0 . . 41 KB . . Zwarburg . . 15:57, 1 October 2012
- (download) PECVD2-SiN-Recipe-100SiH4-100C-Medium-Stress.pdf . . 0 × 0 . . 41 KB . . Zwarburg . . 15:57, 1 October 2012
- (download) PECVD2-SiN-Recipe-120W-100C-Low-Stress.pdf . . 0 × 0 . . 41 KB . . Zwarburg . . 17:18, 17 August 2012
- (download) PECVD2-SiN-Recipe-120W-250C-Low-Stress.pdf . . 0 × 0 . . 41 KB . . Zwarburg . . 16:20, 20 August 2012
- (download) PECVD2-SiN-Recipe-120W-50C-Low-Stress.pdf . . 0 × 0 . . 41 KB . . Zwarburg . . 17:37, 17 August 2012
- (download) PECVD2-SiN-Recipe-50W-100C-Medium-Stress.pdf . . 0 × 0 . . 41 KB . . Zwarburg . . 17:17, 17 August 2012
- (download) PECVD2-SiN-Recipe-50W-250C-Medium-Stress.pdf . . 0 × 0 . . 41 KB . . Zwarburg . . 16:19, 20 August 2012
- (download) PECVD2-SiN-Recipe-50W-50C-Medium-Stress.pdf . . 0 × 0 . . 41 KB . . Zwarburg . . 17:37, 17 August 2012
- (download) PECVD2-SiN-Recipe-5W-100C-High-Stress.pdf . . 0 × 0 . . 41 KB . . Zwarburg . . 17:17, 17 August 2012