Dry Etching Recipes
RIE Etching
ICP Etching
Oxygen Plasma Systems
Other Dry Etchers
Material
RIE 1
(Retired)
RIE 2
(MRC)
RIE 3
(MRC)
RIE 5
(PlasmaTherm)
Si Deep RIE
(PTI/Bosch)
ICP Etch 1
(Panasonic 1)
ICP Etch 2
(Panasonic 2)
ICP-Etch
(Unaxis VLR)
Ashers
(Technics PEII)
Plasma Clean
(Gasonics 2000)
UV Ozone Reactor
Plasma Activation
(EVG 810)
XeF2 Etch
(Xetch)
Vapor HF Etch
(uETCH)
CAIBE
(Oxford)
Al
A
R1
R1
Ti
R1
A
Cr
A
R1
A
Ge
Ag
Pt
R1
Au
R1
Ni
R1
Cu
Ru
Mo
Ta
W-TiW
R1
A
Al
2
O
3
HfO
2
ITO
R1
SiO
2
R1
R1
R1
SiN
R1
R1
SiOxNy
Ta
2
O
5
TiO
2
TiN
ZnO
2
ZrO
2
GaAs
R1
R1
R1
GaAs-AlGaAs Etch (Unaxis VLR)
AlGaAs
R1
R1
GaAs-AlGaAs Etch (Unaxis VLR)
InGaAlAs
InP-InGaAsP-InGaAlAs Etching (RIE 2)
InP-InGaAs-InAlAs Etch (Unaxis VLR)
InGaAsP
InP-InGaAsP-InGaAlAs Etching (RIE 2)
InP-InGaAs-InAlAs Etch (Unaxis VLR)
InP
InP-InGaAsP-InGaAlAs Etching (RIE 2)
InP-InGaAs-InAlAs Etch (Unaxis VLR)
GaN
GaN Etch (RIE 5)
R1
R1
AlGaN
R1
AlN
R1
GaSb
CdZnTe
R1
ZnS
R1
ZnSe
R1
Si
R1
R1
SiC
R1
A
Sapphire
R1
A
Material
RIE 1
(Retired)
RIE 2
(MRC)
RIE 3
(MRC)
RIE 5
(PlasmaTherm)
Si Deep RIE
(PlasmaTherm/Bosch Etch)
ICP Etch 1
(Panasonic E626I)
ICP Etch 2
(Panasonic E640)
ICP-Etch
(Unaxis VLR)
Ashers
(Technics PEII)
Plasma Clean
(Gasonics 2000)
UV Ozone Reactor
Plasma Activation
(EVG 810)
XeF2 Etch
(Xetch)
Vapor HF Etch
(uETCH)
CAIBE
(Oxford)
Category
:
Processing
Navigation menu
Personal tools
Create account
Log in
Namespaces
Page
Discussion
English
Views
Read
View source
View history
More
Search
InvisibleMenu
QuickLinks
Lab Rules
Common Questions/FAQ
Staff List
Equipment Signup
Chemicals + MSDS
Protofab
Equipment
Full Tool List
Lithography
Vacuum Deposition
Dry Etch
Wet Processing
Thermal Processing
Packaging
Metrology & Test
Recipes and Data
Lithography
Vacuum Deposition
Dry Etching
Wet Etching
Thermal Processing
Packaging Tools
Data + Info
Process Control Data
Tutorials
Calculators/Utilities
NanoFab Info
Research + Pubs
Tech Talks
Tools
What links here
Related changes
Special pages
Printable version
Permanent link
Page information