Dry Etching Recipes
RIE Etching
ICP Etching
Oxygen Plasma Systems
Other Dry Etchers
Material
RIE 1
(Retired)
RIE 2
(MRC)
RIE 3
(MRC)
RIE 5
(PlasmaTherm)
Si Deep RIE
(PTI/Bosch)
ICP Etch 1
(Panasonic 1)
ICP Etch 2
(Panasonic 2)
ICP-Etch
(Unaxis VLR)
Ashers
(Technics PEII)
Plasma Clean
(Gasonics 2000)
UV Ozone Reactor
Plasma Activation
(EVG 810)
XeF2 Etch
(Xetch)
Vapor HF Etch
(uETCH)
CAIBE
(Oxford)
Al
A
R1
R1
Ti
R1
A
Cr
A
R1
A
Ge
Ag
Pt
R1
Au
R1
Ni
R1
Cu
Ru
Mo
Ta
W-TiW
R1
A
Al
2
O
3
HfO
2
ITO
R1
SiO
2
R1
R1
R1
SiN
R1
R1
SiOxNy
Ta
2
O
5
TiO
2
TiN
ZnO
2
ZrO
2
GaAs
R1
R1
R1
GaAs-AlGaAs Etch (Unaxis VLR)
AlGaAs
R1
R1
GaAs-AlGaAs Etch (Unaxis VLR)
InGaAlAs
InP-InGaAsP-InGaAlAs Etching (RIE 2)
InP-InGaAs-InAlAs Etch (Unaxis VLR)
InGaAsP
InP-InGaAsP-InGaAlAs Etching (RIE 2)
InP-InGaAs-InAlAs Etch (Unaxis VLR)
InP
InP-InGaAsP-InGaAlAs Etching (RIE 2)
InP-InGaAs-InAlAs Etch (Unaxis VLR)
GaN
GaN Etch (RIE 5)
R1
R1
AlGaN
R1
AlN
R1
GaSb
GaSb Etch Unaxis VLR)
CdZnTe
R1
ZnS
R1
ZnSe
R1
Si
R1
R1
SiC
R1
A
Sapphire
R1
A
Material
RIE 1
(Retired)
RIE 2
(MRC)
RIE 3
(MRC)
RIE 5
(PlasmaTherm)
Si Deep RIE
(PlasmaTherm/Bosch Etch)
ICP Etch 1
(Panasonic E626I)
ICP Etch 2
(Panasonic E640)
ICP-Etch
(Unaxis VLR)
Ashers
(Technics PEII)
Plasma Clean
(Gasonics 2000)
UV Ozone Reactor
Plasma Activation
(EVG 810)
XeF2 Etch
(Xetch)
Vapor HF Etch
(uETCH)
CAIBE
(Oxford)
Category
:
Processing
Navigation menu
Personal tools
Create account
Log in
Namespaces
Page
Discussion
English
Views
Read
View source
View history
More
Search
InvisibleMenu
QuickLinks
Lab Rules
Common Questions/FAQ
Staff List
Equipment Signup
Chemicals + MSDS
Protofab
Equipment
Full Tool List
Lithography
Vacuum Deposition
Dry Etch
Wet Processing
Thermal Processing
Packaging
Metrology & Test
Recipes and Data
Lithography
Vacuum Deposition
Dry Etching
Wet Etching
Thermal Processing
Packaging Tools
Data + Info
Process Control Data
Tutorials
Calculators/Utilities
NanoFab Info
Research + Pubs
Tech Talks
Tools
What links here
Related changes
Special pages
Printable version
Permanent link
Page information