About

The Filmetrics F40-UV is a microscope-mounted thin-film measurement system, allowing you to non-descructively measure thin-film thicknesses in small (patterned) areas on your sample. It is an optical reflectometer, acquiring reflection spectra between 400-900nm optical wavelengths (Vis to Near-IR) with a regular halogen microscope light source. The Filmetrics software then performs curve-fitting to determine the thickness and/or refractive index of the measured films.

It is equipped with 10x, 20x, 50x, 100x and 150x objectives.