Photoluminescence PL Setup (Custom)
|
In Progress - incomplete info.
About
The Photoluminescence setup is on the same optical table as the Hologaphic Lithography setup.
Detailed Specifications
Pump Lasers Available
325nm He-Cd - single mode, spatially filtered
405nm Diode Laser
660nm Diode Laser