PECVD Recipes

From UCSB Nanofab Wiki
Revision as of 19:32, 22 November 2019 by John d (talk | contribs) (SiN deposition (Unaxis VLR): SiN recipes under development)
Jump to navigation Jump to search

Back to Vacuum Deposition Recipes.

PECVD 1 (PlasmaTherm 790)

Note: Software upgrade performed on 2018-10-10. Note any changes in film.


SiN deposition (PECVD #1)


SiO2 deposition (PECVD #1)


OTHER recipes: Low-Stress (LS) SiN and SiOxNy deposition (PECVD #1)

PECVD 2 (Advanced Vacuum)

SiO2 deposition (PECVD #2)


SiN deposition (PECVD #2)



Low-Stress SiN deposition (PECVD #2)

Low-Stress SilIcon Nitride (< 100 MPa)


Amorphous-Si deposition (PECVD #2)

ICP-PECVD (Unaxis VLR)

SiN deposition (Unaxis VLR)

These Si3N4 recipes are not valid currently, and are still under development. 
-- Demis 2019-11-22

SiO2 deposition (Unaxis VLR)