YES Recipe Screenshots: STD-N2-O2
From UCSB Nanofab Wiki
Revision as of 19:08, 30 November 2023 by
John d
(
talk
|
contribs
)
(screenshots of "STD-N2-O2-100C-0.7KW-15sec" and "STD-N2-O2-180C-3KW-1min")
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)
Jump to navigation
Jump to search
STD-N2-O2-180C-3KW-1min
Header
Steps
STD-N2-O2-180C-3KW-1min - header
STD-N2-O2-180C-3KW-1min - steps
STD-N2-O2-100C-0.7KW-15sec
Header
Steps
STD-N2-O2-100C-0.7KW-15sec - header
STD-N2-O2-100C-0.7KW-15sec - steps
Navigation menu
Personal tools
Create account
Log in
Namespaces
Page
Discussion
English
Views
Read
View source
View history
More
Search
InvisibleMenu
QuickLinks
Lab Rules
Common Questions/FAQ
Staff List
Equipment Signup
Chemicals + MSDS
Protofab
Equipment
Full Tool List
Lithography
Vacuum Deposition
Dry Etch
Wet Processing
Thermal Processing
Packaging
Metrology & Test
Recipes and Data
Lithography
Vacuum Deposition
Dry Etching
Wet Etching
Thermal Processing
Packaging Tools
Data + Info
Process Control Data
Tutorials
Calculators/Utilities
NanoFab Info
Research + Pubs
Tech Talks
Tools
What links here
Related changes
Special pages
Printable version
Permanent link
Page information