File:PRStrip 019 (1).jpg
Size of this preview: 748 × 600 pixels. Other resolution: 1,280 × 1,026 pixels.
Original file (1,280 × 1,026 pixels, file size: 845 KB, MIME type: image/jpeg)
Summary
Si Etch FICP 9/19/24
File history
Click on a date/time to view the file as it appeared at that time.
| Date/Time | Thumbnail | Dimensions | User | Comment | |
|---|---|---|---|---|---|
| current | 16:23, 30 September 2024 | 1,280 × 1,026 (845 KB) | Noahdutra (talk | contribs) | Si Etch FICP 9/19/24 |