RIE Etching Recipes

From UCSB Nanofab Wiki
Revision as of 03:13, 17 July 2026 by John d (talk | contribs) (→Photoresist and ARC (RIE 5))
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)
Jump to navigation Jump to search

Back to Dry Etching Recipes.

RIE 2 (MRC)

CdZnTe Etching (RIE 2)

ZnS Etching (RIE 2)

ITO Etching (RIE 2)

InP-InGaAsP-InGaAlAs Etching (RIE 2)

RIE 5 (PlasmaTherm)

AlGaAs\GaAs Etching (RIE 5)

GaN Etching (RIE 5)

Photoresist and ARC (RIE 5)

DUV42P (AR2) etching

  • O2 = 20sccm // Pressure = 10mT // RF = 100W // Time = 40 sec
  • No need to pump/purge, can etch right away
  • No helium cooling
  • Can run in manual mode