Stepper 3 (ASML DUV)

From UCSB Nanofab Wiki
Revision as of 00:43, 28 June 2012 by Zwarburg (talk | contribs) (Created page with "{{tool|{{PAGENAME}} |picture=ASML.jpg |type = Vacuum Deposition |super= Adam Abrahamsen |phone=(805)839-3918x213 |location=Bay 3 |email=abrahamsen@ece.ucsb.edu |description = ASM…")
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)
Jump to navigation Jump to search
Stepper 3 (ASML DUV)
Tool Type Vacuum Deposition
Location Bay 3
Description ASML PAS S500/300 DUV Stepper
Manufacturer ASML
Vacuum Deposition Recipes



About

The ASML DUV stepper is a 248nm line stepper for imaging dense features down to below 200nm and isolated line structures down to below 150nm. The system is a variable NA system and has a field image size of 21 x 21mm for 0.63 NA and a field size of 22mm x 27mm for 0.4 to 0.57NA. Overlay accuracy is better than 30nm. The system is configured for 4” wafers and pieces down to 14mm in size can be exposed using a 4” wafer as a carrier.