Tube Furnace (Tystar 8300)

From UCSB Nanofab Wiki
Revision as of 00:47, 26 September 2013 by Ray t (talk | contribs) (→See Also)
Jump to navigation Jump to search
Tube Furnace (Tystar 8300)
Tool Type Thermal Processing
Location Bay 4
Supervisor Tony Bosch
Supervisor Phone (805) 893-3486
Supervisor E-Mail bosch@ece.ucsb.edu
Description Tystar 8" 3-Tube Oxidation/Annealing System
Manufacturer Tystar Corporation
Sign up for this tool


About

The three stack Tystar 8” furnace is used primarily for 3 processes. The processes are dedicated for one tube each:

  1. SOG curing - Tube 1
  2. Dry or wet oxidation of silicon - Tubes 2 and 3
  3. General furnace annealing - Tube 3

The tubes can hold up to one hundred 8” wafers per tube per cycle. We have boats for various wafer sizes, including pieces. The maximum temperature is 1050°C for the system. Gases used are O2, Steam from DI-H2O, N2.

Useful Information

Tystar Wafer Boat Drawing - 4" Wafer with 0.5mm Slots

See Also