Difference between revisions of "Automated Coat/Develop System (S-Cubed Flexi)"
Jump to navigation
Jump to search
(added PR's and links to recipes) |
(added notice abotu staff use only) |
||
Line 10: | Line 10: | ||
|materials = |
|materials = |
||
|toolid= |
|toolid= |
||
− | }} |
+ | }} |
+ | '''This tool is only available for Staff use at this time.''' |
||
+ | |||
=About= |
=About= |
||
Line 35: | Line 37: | ||
*Recipe Page for S-Cubed Coater: [[Lithography Recipes#Automated%20Coat.2FDevelop%20System%20Recipes%20.28S-Cubed%20Flexi.29|Lithography Recipes > Automated Coat/Develop System Recipes (S-Cubed Flexi]]) |
*Recipe Page for S-Cubed Coater: [[Lithography Recipes#Automated%20Coat.2FDevelop%20System%20Recipes%20.28S-Cubed%20Flexi.29|Lithography Recipes > Automated Coat/Develop System Recipes (S-Cubed Flexi]]) |
||
+ | *See the [https://www.nanotech.ucsb.edu/wiki/index.php/Lithography_Recipes#Chemicals_Stocked_.2B_Datasheets Photolith. Chemicals page] for info on the installed resists. |
||
=Operating Procedures= |
=Operating Procedures= |
Revision as of 16:03, 8 October 2019
|
This tool is only available for Staff use at this time.
About
To Be Added
Detailed Specifications
- Wafer Size: 100mm (150mm possible but not set up)
- PR Coating Properties:
- Uniformity < 1.0%
- < 100 particles on 100mm wafer
- Photoresists/Underlayers Available:
- UV6-0.8
- DS-K101-304
- PMMA
- PMGI SF11
- PMGI SF5
- Solvents Available:
- EBR100
- Developers Available:
- AZ 300 MiF
Process Information
- Recipe Page for S-Cubed Coater: Lithography Recipes > Automated Coat/Develop System Recipes (S-Cubed Flexi)
- See the Photolith. Chemicals page for info on the installed resists.
Operating Procedures
- To Be Added