File:IBD 9-period DBR - Reflectivity Spectrum (EMpy).png

From UCSB Nanofab Wiki
Revision as of 12:43, 31 March 2022 by John d (talk | contribs)
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)
Jump to navigation Jump to search

IBD_9-period_DBR_-_Reflectivity_Spectrum_(EMpy).png(706 × 566 pixels, file size: 56 KB, MIME type: image/png)

IBD DBR calibration example - test-DBR dep 9-periods SiO/TaO after Fabry-perot correction method.