File:Oxford Etcher - InP Grating Etch at 20 C - Oxford Cobra 300 2021-08-26.pdf

From UCSB Nanofab Wiki
Revision as of 13:55, 8 October 2021 by John d (talk | contribs) (Oxford Etcher - InP Grating Etch at 20 C - Oxford Cobra 300 2021-08-26 Ning Cao)
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)
Jump to navigation Jump to search

Oxford_Etcher_-_InP_Grating_Etch_at_20_C_-_Oxford_Cobra_300_2021-08-26.pdf(file size: 1.38 MB, MIME type: application/pdf)

Summary

Oxford Etcher - InP Grating Etch at 20 C - Oxford Cobra 300 2021-08-26 Ning Cao

File history

Click on a date/time to view the file as it appeared at that time.

Date/TimeDimensionsUserComment
current18:35, 5 March 2024 (1.38 MB)John d (talk | contribs)added temp and carrier to recipe page
18:33, 5 March 2024 (1.37 MB)John d (talk | contribs)fixed typo in std recipe name
18:22, 5 March 2024 (1.37 MB)John d (talk | contribs)v2, added "std" recipe on top slide.
13:55, 8 October 2021 (1.32 MB)John d (talk | contribs)Oxford Etcher - InP Grating Etch at 20 C - Oxford Cobra 300 2021-08-26 Ning Cao

The following page uses this file: