File:Oxford Etcher - InP Grating Etch at 20 C - Oxford Cobra 300 2021-08-26.pdf
Revision as of 18:35, 5 March 2024 by John d (talk | contribs) (John d uploaded a new version of File:Oxford Etcher - InP Grating Etch at 20 C - Oxford Cobra 300 2021-08-26.pdf)
Oxford_Etcher_-_InP_Grating_Etch_at_20_C_-_Oxford_Cobra_300_2021-08-26.pdf (file size: 1.38 MB, MIME type: application/pdf)
Summary
Oxford Etcher - InP Grating Etch at 20 C - Oxford Cobra 300 2021-08-26 Ning Cao
File history
Click on a date/time to view the file as it appeared at that time.
Date/Time | Dimensions | User | Comment | |
---|---|---|---|---|
current | 18:35, 5 March 2024 | (1.38 MB) | John d (talk | contribs) | added temp and carrier to recipe page |
18:33, 5 March 2024 | (1.37 MB) | John d (talk | contribs) | fixed typo in std recipe name | |
18:22, 5 March 2024 | (1.37 MB) | John d (talk | contribs) | v2, added "std" recipe on top slide. | |
13:55, 8 October 2021 | (1.32 MB) | John d (talk | contribs) | Oxford Etcher - InP Grating Etch at 20 C - Oxford Cobra 300 2021-08-26 Ning Cao |
You cannot overwrite this file.
File usage
The following page uses this file: