File:Oxford Etcher - InP Ridge Etch using Oxford PlasmaPro 100 Cobra - 2021-09-08.pdf
Revision as of 18:43, 5 March 2024 by John d (talk | contribs) (John d uploaded a new version of File:Oxford Etcher - InP Ridge Etch using Oxford PlasmaPro 100 Cobra - 2021-09-08.pdf)
Oxford_Etcher_-_InP_Ridge_Etch_using_Oxford_PlasmaPro_100_Cobra_-_2021-09-08.pdf (file size: 1.46 MB, MIME type: application/pdf)
Summary
Oxford Etcher - InP Ridge Etch using Oxford PlasmaPro 100 Cobra - 2021-09-08 Ning Cao, 2021-09-08
File history
Click on a date/time to view the file as it appeared at that time.
Date/Time | Dimensions | User | Comment | |
---|---|---|---|---|
current | 18:43, 5 March 2024 | (1.46 MB) | John d (talk | contribs) | added info abotu :stadnard" recipe, name, mounting method etc. |
13:59, 8 October 2021 | (1.45 MB) | John d (talk | contribs) | Oxford Etcher - InP Ridge Etch using Oxford PlasmaPro 100 Cobra - 2021-09-08 Ning Cao, 2021-09-08 |