- Heat up lower substrate on hotplate at 135°C
- Apply XYZ grams of crystalbond wax, with stick, to the surface. Spread so that enough wax is present so that entire underside of upper substrate will be in contact with wax. Remove from hotplate and cool. If wax got on the underside, can spin face-down on POLOS spinner @ 2000rpm with ACE squirt bottle to remove.
- Place carrier wafer on Logitech bonder surface, wax face-up.
- Place sample to be bonded on top
- Place 110mm chemical filter paper on top
- Close lid, secure lid clamp
- Run recipe:
- XYZ °C
- XYZ seconds
- Vacuum etc.?