File:IBD SiON - Dep rate vs O2 flow - wiki.png
Jump to navigation
Jump to search
IBD_SiON_-_Dep_rate_vs_O2_flow_-_wiki.png (643 × 374 pixels, file size: 38 KB, MIME type: image/png)
Dep rate of IBD SiOxNy vs. Assist Beam Oxygen flow.