File:PECVD1 SiO2 F50 WaferMap example.jpg
Jump to navigation
Jump to search
![File:PECVD1 SiO2 F50 WaferMap example.jpg](/w/images/thumb/c/cd/PECVD1_SiO2_F50_WaferMap_example.jpg/581px-PECVD1_SiO2_F50_WaferMap_example.jpg?20250207005003)
Size of this preview: 581 × 599 pixels. Other resolution: 1,541 × 1,590 pixels.
Original file (1,541 × 1,590 pixels, file size: 1.04 MB, MIME type: image/jpeg)
Screenshot of Filmetrics F50 wafermap of typical DepCals film
File history
Click on a date/time to view the file as it appeared at that time.
Date/Time | Thumbnail | Dimensions | User | Comment | |
---|---|---|---|---|---|
current | 00:50, 7 February 2025 | ![]() | 1,541 × 1,590 (1.04 MB) | John d (talk | contribs) |