21:41, 21 August 2025 W Film by DC Sputtering sputter3.pdf (file) 1.5 MB   2
21:38, 21 August 2025 TiW Film by DC Co-Sputtering in Sputter3.pdf (file) 1.45 MB TiW cosputtering from W target and TiW (10wt%Ti) target 1
23:31, 9 June 2023 Gas mixture comparison.jpg (file) 136 KB   1
23:17, 9 June 2023 Au oxidation by O2-N2 ash.jpg (file) 124 KB   1
16:39, 5 June 2023 PPR 220-7 Etch Rates vs Temperature.jpg (file) 68 KB   1
16:34, 5 June 2023 PPR220-7 Etch Rates vs Temperature.jpg (file) 52 KB   1
16:28, 5 June 2023 PPR220-7 Etch Rates (nm min) vs. Temp(C) Recipe STD O2only 3KW-3min-Temp (1).png (file) 26 KB   1
16:19, 5 June 2023 PPR220-7 Etch Rates (nm min) vs. Temp(C) Recipe STD O2only 3KW-3min-Temp.png (file) 20 KB   1