Dry Etching Recipes: Difference between revisions

From UCSB Nanofab Wiki
Jump to navigation Jump to search
(fixed CAIBE recipe link)
(linked PR&ARC etchign to ICP1 & RIE5 sections)
Line 519: Line 519:
|
|
|A
|A
|[https://www.nanotech.ucsb.edu/wiki/index.php/RIE_Etching_Recipes#Photoresist_and_ARC R]
|A
|
|
|
|
|[https://www.nanotech.ucsb.edu/wiki/index.php/ICP_Etching_Recipes#Photoresist_and_ARC_Etching R]
|A
|[https://www.nanotech.ucsb.edu/wiki/index.php/ICP_Etching_Recipes#Photoresist_and_ARC_etching R]
|[https://www.nanotech.ucsb.edu/wiki/index.php/ICP_Etching_Recipes#Photoresist_and_ARC_etching R]
|
|

Revision as of 01:13, 29 September 2018

  • R = Recipe is available. Clicking this link will take you to the recipe.
  • A = Material is available for use, but no recipes are provided.
Dry Etching Recipes
RIE Etching ICP Etching Oxygen Plasma Systems Other Dry Etchers
Material RIE 1
(Retired)
RIE 2
(MRC)
RIE 3
(MRC)
RIE 5
(PlasmaTherm)
DSEIII
(PlasmaTherm)
SLR Fluorine ICP (PlasmaTherm) ICP Etch 1
(Panasonic 1)
ICP Etch 2
(Panasonic 2)
ICP-Etch
(Unaxis VLR)
Ashers
(Technics PEII)
Plasma Clean
(Gasonics 2000)
UV Ozone Reactor Plasma Activation
(EVG 810)
XeF2 Etch
(Xetch)
Vapor HF Etch
(uETCH)
CAIBE
(Oxford)
Ag
Al A R1 R1
Au A
Cr A R1 A
Cu
Ge A
Mo
Ni R1
Pt R1
Ru
Si R1 A R1
Ta
Ti R1 A
Al2O3 R
Al2O3 (Sapphire) R1 A
AlGaAs R1 R1 GaAs-AlGaAs Etch (Unaxis VLR)
AlGaN R1
AlN R1
CdZnTe R1
GaAs R1 R1 R1 GaAs-AlGaAs Etch (Unaxis VLR)
GaN R1 R1 R1
GaSb A GaSb Etch Unaxis VLR)
HfO2
InGaAlAs InP-InGaAsP-InGaAlAs Etching (RIE 2) InP-InGaAs-InAlAs Etch (Unaxis VLR)
InGaAsP InP-InGaAsP-InGaAlAs Etching (RIE 2) InP-InGaAs-InAlAs Etch (Unaxis VLR)
InP InP-InGaAsP-InGaAlAs Etching (RIE 2) A A InP-InGaAs-InAlAs Etch (Unaxis VLR)
ITO R1
Photoresist

& ARC

A R R R A A
SiC R1 A
SiN SiNx Etching (RIE 3) R1 R1 A
SiO2 SiO2 Etching (RIE 3) A R1 R1 R1
SiOxNy A A
Ta2O5 A
TiN
TiO2
W-TiW R1 A
ZnO2
ZnS R1
ZnSe R1
ZrO2
Material RIE 1
(Retired)
RIE 2
(MRC)
RIE 3
(MRC)
RIE 5
(PlasmaTherm)
DSEIII
(PlasmaTherm)
SLR Fluorine ICP (PlasmaTherm) ICP Etch 1
(Panasonic E626I)
ICP Etch 2
(Panasonic E640)
ICP-Etch
(Unaxis VLR)
Ashers
(Technics PEII)
Plasma Clean
(Gasonics 2000)
UV Ozone Reactor Plasma Activation
(EVG 810)
XeF2 Etch
(Xetch)
Vapor HF Etch
(uETCH)
CAIBE
(Oxford)